Hostname: page-component-54dcc4c588-5q6g5 Total loading time: 0 Render date: 2025-10-10T03:59:34.854Z Has data issue: false hasContentIssue false

Surface Deformation Nanostructures and Stress Corrosion Crack Precursors Originating from Surface Grinding

Published online by Cambridge University Press:  01 February 2011

Matthew Olszta
Affiliation:
matthew.olszta@pnl.govolszta77@gmail.com
Larry Thomas
Affiliation:
larry.thomas@pnl.gov, Pacific Northwest National Laboratory, Richland, United States
Stephen Bruemmer
Affiliation:
stephen.bruemmer@pnl.gov, Pacific Northwest National Laboratory, Richland, United States
Get access

Abstract

Stress corrosion cracking (SCC) in light water reactor components has long been studied from a post mortem perspective, yielding insights into water chemistries and effects on crack propagation. Analysis of a cracked component does not effectively provide information on the corrosion events or on SCC initiation. It is important that microstructures of these early stages be understood because the original surface of the component formed during fabrication is often not the final surface condition that is exposed to reactor water. Pre-service grinding of reactor components and welds is performed for a variety of reasons, from aesthetics to preparation for non-destructive testing. It is this final surface microstructure that often controls SCC initiation. Surface and near-surface characteristics have been investigated in 304SS metal coupons on which controlled grinding was performed. These examinations indicate the extent of subsurface microstructural damage before high-temperature water exposure. Analytical electron microscopy techniques have been used to gain insights into possible surface precursors to corrosion damage and SCC initiation.Nanocrystalline grains were commonly found at the surface in lightly ground to heavily abraded materials within the first ˜0.5-10 ųm along with high dislocation densities, twinning and lath structures.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Suzuki, S. Takamori, K. Kumagai, K. Fukuda, T. Yamashita, Y. and Futami, T.Evaluation of SCC Morphology on L-Grade Stainless Steel in BWRs,” J. High Pressure Institute of Japan, 42–4 (2004) 197.Google Scholar
2 Ooki, S. Tanaka, Y. Takamori, K. Suzuki, S. Tanaka, T. Saito, Y. Nakamura, T. Kato, T. Chatani, K. and Komoda, M. Proc. 12th Int. Symp. Environmental Degradation of Materials in Nuclear Power Systems Water Reactors, National Association of Corrosion Engineers, 2005, p. 365.Google Scholar
3 Olszta, M.J. Thomas, L.E. Bruemmer, S.M. 14th Int. Symp. Environmental Degradation of Materials in Nuclear Power Systems Water Reactors, National Association of Corrosion Engineers, 2009, in press.Google Scholar
4 Thomas, L.E. Edwards, D. Asano, K. Ooki, S. Bruemmer, S. “Crack-Tip Characterizations in BWR Service Components,” Proc. 13th Inter. Conference on Env. Deg. of Materials in Nuclear Power Systems, Whistler, B.C., 2007.Google Scholar
6 Bruemmer, S. M. and Thomas, L. E.High-Resolution Characterizations of Stress-Corrosion Cracks in Austenitic Stainless Steel from Crack Growth Tests in BWR-Simulated Environments,” ibid 3, p. 189.Google Scholar
7 Thomas, L. E. and Bruemmer, S. M. “Comparison of IGSCC Crack-Tip Characteristics in BWR Oxidizing Water and BWR Hydrogen Water Chemistry Conditions,” ibid 6.Google Scholar
8 Staehle, R. W. personal communication from “Overview of Initiation of SCC in Fe-Cr-Ni Alloys,” Presented at International Cooperative Group on Environment-Assisted Cracking, Bastad, Sweden, 2008.Google Scholar