Role of Heat Treating on the Intergranular Stress Corrosion Cracking of Alloy 600

Published online by Cambridge University Press:  01 February 2011

A. Aguilar
Affiliation:
Instituto de Ciencias Físicas, UNAM. A.P. 48–3, C.P. 62251, Cuernavaca, Morelos, México
A. García-Ruiz
Affiliation:
UPIICSA-COFAA, Instituto Politécnico Nacional (IPN). Té 950, Col. Granjas-México, Iztacalco, 08400, México, D.
A. Escobedo
Affiliation:
Instituto de Ciencias Físicas, UNAM. A.P. 48–3, C.P. 62251, Cuernavaca, Morelos, México
R. Pérez
Affiliation:
Centro de Física Aplicada y Tecnología Avanzada, Universidad Nacional Autónoma de México, P. O. Box 1–1010, C.P. 76230, Boulevard Juriquilla 3001, Santiago de Querétaro, Qro. México. Email: andres@fis.unam.mx
Get access

Abstract

It has been recognized in Ni-base alloys that the grain boundary chemistry and its microestructural heterogeneities are important factors in the material environmental degradation. Therefore, in this study, we investigated the role of the heat treatments and the obtained microstructure in the IGSCC susceptibility of alloy 600 in environments of pressurized water reactors (PWR). The role of microstructure on the intergranular cracking resistance (IGC) of alloy 600 was also investigated using a modified wedge opening loading specimens which were annealed at 930, 800 and 600°C and also exposed to high purity water pressurized with hydrogen at 300°C. It was found the microstructure induce relatively low crack growth rates associated with the development of significant plastic deformation at the crack tip. In addition, some common features were found between the IGSCC performance and the pre-fatigue cracking conditions. For this purpose, the fatigue crack growth properties of this alloy were also evaluated using the ASTM E 606–92.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Environmental Degradation of Materials in Nuclear Power Systems-Water Reactor, Proc. Third Intl. Symp. Traverse City, Michigan, TMS (1988), p. 551.Google Scholar
2. Shen, C. H. and Shewmon, P. G., Metall. Trans. A, 21A, 1261(1990).Google Scholar
3. Lenartova, I., Habashi, M., Vodarek, V., Galland, J., Tvrdy, M. and Hyspecka, L., Int. Conf. on Corrosion–Deformation Interactions, Eurocorr'96, Nice France, Sept. 24–26, pp. 5–1(1996).Google Scholar
4. Newman, C. and Saito, M., Corrosion–deformation interactions, CDI-9, Conf. Proc., Fontainebleau-France, Oct. 5–7, 1992, Les editions de physique, (1992), p. 3.Google Scholar
5. Rebak, R.B., Szklarska-Smialowska, Z., Corrosion Vol. 47, No. 10, 755 (1991).Google Scholar
6. Shen, C.H., Shewmon, P.G., Met. Trans. 21A 1261 (1990).Google Scholar
7. Shewmon, P.G. and Shen, Y., Metall. Trans. A. Vol. 22A, 1857 (1991).Google Scholar
8. Magnin, T., Renaudot, N., Foct, F., Materials Transactions, JIM, 210 (2000).Google Scholar
9. Taylor, D.F., Corrosion, Vol.35, 550 (1999).Google Scholar
10. Novak, S. R. and Rolfe, S. T.. Journal of Materials Vol. 4, No. 3, 701 (1969).Google Scholar
11. Deans, W. F. and Richards, C. E.. Journal of Testing and Evaluation, 7 147 (1979).Google Scholar
12. Bruemmer, S.M., Charlot, L.A., Henager, C.H. Jr., Corrosion Science, 782 (1988).Google Scholar
13. Uhlemann, M., Pound, B.G., Corrosion Science, 40–4/5 645 (1998).Google Scholar
14. Delafosse, D., Magnin, T., Eng. Fract. Mech. 68–6, 693(2001).Google Scholar