Nanoindentation Study of Very Low Stress Plasticity

Published online by Cambridge University Press:  10 February 2011

J. Woirgard
Affiliation:
Laboratoire de Métallurgie Physique, U.M.R. C.N.R.S. 6630, Université de Poitiers Bat SP2MI, BP 179, 86960 Futuroscope Cedex, France.
C. Tromas
Affiliation:
Laboratoire de Métallurgie Physique, U.M.R. C.N.R.S. 6630, Université de Poitiers Bat SP2MI, BP 179, 86960 Futuroscope Cedex, France.
V. Audurier
Affiliation:
Laboratoire de Métallurgie Physique, U.M.R. C.N.R.S. 6630, Université de Poitiers Bat SP2MI, BP 179, 86960 Futuroscope Cedex, France.
J.C. Girard
Affiliation:
Laboratoire de Métallurgie Physique, U.M.R. C.N.R.S. 6630, Université de Poitiers Bat SP2MI, BP 179, 86960 Futuroscope Cedex, France.
Get access

Abstract

The early stages of plasticity have been studied by nanoindentation at room temperature, with a new apparatus, in GaAs and MgO single crystals. On both materials a very well defined pop-in has been observed, whose characteristics depends on the initial dislocation density in the indented zone. On (100) cleaved surfaces of MgO crystals, several special surface features, including the presence of rosette arms, have been observed by SFM. Starting from these observations a dislocation mechanism has been proposed.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Oliver, W.C. and Pharr, G.M., J. Mat. Res., 7, (1992), p. 15641583.Google Scholar
2. Woirgard, J. and Dargenton, J.C., Meas. Sci. Technol., 6 (1995), p.1621.Google Scholar
3. Dargenton, J.C. and Woirgard, J., Journ. Phys III, 6 (1996), p. 12471260.Google Scholar
4. Strojny, A., Lilleodden, E.T., Wang, G., Sivertsen, J.V. and Gerberich, W.W., Mat. Res. Soc. Symp. Proc., 436, (1997), p. 281286.Google Scholar
5. Corcoran, S.G., Colton, R.J., Lilleodden, E.T. and Geberich, W.W., Mat. Res. Soc. Symp.Proc., 436, (1997), p. 159163.Google Scholar
6. Mann, A. and Pethica, J.B., Mat. Res. Soc. Symp. Proc., 436, (1997), p. 153158.Google Scholar
7. Syed Asif, S.A. and Pethica, J.B., Phil. Mag., 76, (1997), p. 11051118.Google Scholar
8. Bhushan, B., Kulkarni, A., Phil. Mag., 74, (1996), p. 11171128.Google Scholar
9. Geberich, W.W., Venkataraman, S.K., Huang, H., Harvey, S.E. and Kohlstedt, D.L., Acta Metall. Mater., 43, (1995), p. 15691576.Google Scholar
10. Page, T.F., Oliver, W.C. and McHargue, C.J., J. Mat. Res., 7, (1992), p. 450473.Google Scholar
11. Lilleodden, E., Zagrebelny, A.V., Ramamurthy, S. and Carter, C.B., Mat. Res. Soc. Symp. Proc., 436, (1997), p. 177182.Google Scholar
12. Armstrong, R.W. and Wu, C.C., J. Amer. Ceram. Soc., 61, (1978), p. 102.Google Scholar
13. Tromas, C., Girard, J.C., Audurier, V. and Woirgard, J., submitted to the J. of Mater. Res.Google Scholar