Hostname: page-component-54dcc4c588-br6xx Total loading time: 0 Render date: 2025-10-13T02:49:09.768Z Has data issue: false hasContentIssue false

Nanoindentation of Viscoelastic Materials: Mechanical Properties of Polymer Coatings on Aluminum Substrates

Published online by Cambridge University Press:  10 February 2011

K. B. Yoder
Affiliation:
CEMS Department, University of Minnesota, Minneapolis, MN
S. Ahuja
Affiliation:
Xerox Corporation, Webster, NY
K. T. Dihn
Affiliation:
Xerox Corporation, Webster, NY
D. A. Crowson
Affiliation:
Hysitron Incorporated, Minneapolis, MN
S. G. Corcoran
Affiliation:
Hysitron Incorporated, Minneapolis, MN
L. Cheng
Affiliation:
CEMS Department, University of Minnesota, Minneapolis, MN
W. W. Gerberich
Affiliation:
CEMS Department, University of Minnesota, Minneapolis, MN
Get access

Abstract

The mechanical properties of four polymer coatings on aluminum foil substrates are examined using nanoindentation with a Hysitron Triboscope, an add-on to an AFM. In addition to static hardness and modulus measurements, the viscoelastic properties of the films, which differ in Tg and extent of crosslinking, are investigated by employing two techniques: using nanoindentation parameters to fit the creep response of the material to a one-dimensional equation based on a three-element Zener model of the viscoelastic behavior of the polymer; and fitting the creep response of the material to a previously developed, three-dimensional model of the response of a viscoelastic material to indentation by a spherical indenter. It is found that the measured static moduli are about 1.5 times greater than results of fitting creep data to the 1-D model, and are a factor of 3–6 times greater than those obtained by fits of the 3-D model.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Doerner, M. F. and Nix, W. D., J. Mater. Res. 1, 601 (1986).Google Scholar
2. Oliver, W. C. and Pharr, G. M., J. Mater. Res. 7, 1564 (1992).Google Scholar
3. McCrum, N. G., Buckley, C. P., and Bucknall, C. B., Principles of Polymer Engineering, Oxford University Press, New York, 1995, p. 126.Google Scholar
4. Ward, I. M., Mechanical Properties of Solid Polymers, John Wiley and Sons, New York, 1983, p. 93.Google Scholar
5. Cheng, L., Scriven, L. E., and Gerberich, W. W., In Fundamentals of Nanoindentation and Nanotribology Symposium, MRS Spring Meeting, San Fransisco (1998).Google Scholar
6. L. Cheng (private communication).Google Scholar
7. Yoder, K. B., Stone, D. S., Hoffman, R. A., and Lin, J. C., in press.Google Scholar
8. Tsui, T. Y., Oliver, W. C., and Pharr, G. M., J. Mater. Res. 11, 752 (1996).Google Scholar