Nanoindentation of Silicate Low-K Dielectric Thin Films

Published online by Cambridge University Press:  01 February 2011

Joseph B. Vella
Affiliation:
Motorola, Digital DNATM Labs
Alex A. Volinsky
Affiliation:
Motorola, Digital DNATM Labs
Indira S. Adhihetty
Affiliation:
Motorola, Digital DNATM Labs
N.V. Edwards
Affiliation:
Process and Materials Characterization Lab, Mesa, AZ.
William W. Gerberich
Affiliation:
University of Minnesota, Dept. of Chem. Eng. and Mat. Science, Minneapolis, MN.
Get access

Abstract

The capabilities of nanoindentation to characterize low-k organo silicate glass (OSG) thin films is explored as a relatively rapid and inexpensive metric of mechanical properties, adhesion strength, and fracture toughness. One method of decreasing the static dielectric constant of OSG interlayer dielectrics requires the introduction of porosity in the material which has a dramatic impact on its mechanical and toughness properties. Percolation theory is used to formulate a correlation between porosity and elastic modulus. Using cube corner diamond indentation and scratch testing fracture toughness calculations are also discussed.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Read, D. T., Dally, J.W., J. Mater. Res., 8(7), pp. 15421549 (1993).Google Scholar
2. Weihs, T.P., Hong, S., Bravman, J.C., and Nix, W.D., J. Mater. Res. 3(5), pp. 931942 (1998).Google Scholar
3. Baker, S.P. and Nix, W.D., J. Mater. Res. 9(12), pp. 31313152 (1994).Google Scholar
4. Doerner, M. and Nix, W.D., J. Mater. Res. 1, p. 601 (1986).Google Scholar
5. Pharr, G.M., Oliver, W.C., Brotzen, F., J. Mater. Res., 7 (3), pp. 613617, (1992)Google Scholar
6. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, pp.15641583, (1992)Google Scholar
7. Marshall, D.B. and Evans, A.G., J. Appl. Phys., 56, 2632, (1984)Google Scholar
8. Vlassak, J.J, Drory, M.D. and Nix, W.D., J. Mater. Res., Vol. 12, No. 7, p. 1900, (1997)Google Scholar
9. Kriese, M.D. and Gerberich, W.W., J. Mater. Res., 14 (7), 3007, (1999)Google Scholar
10. Kriese, M.D., Gerberich, W.W, Moody, N.R., J. Mater. Res., 14 (7), 3019, (1999)Google Scholar
11. Volinsky, A.A, Tymiak, N.I., Kriese, M.D, Gerberich, W.W and Hutchinson, J.W., Materials Research Society Symposium Proceedings, Vol. 539, (Pittsburgh, Pennsylvania: Materials Research Society), p. 277, (1999)Google Scholar
12. Phani, K. K. and Niyogi, S. K., J. Mater. Sci., 22 257, (1987)Google Scholar
13. II, E.O. Shaffer, Howard, K.E., Mills, M.E., III, P.H. Townsend, Mat. Sci. Symp. Proc., Vol 612 D1.1, 18, (2000)Google Scholar
14. Xiao, X. et al., Microelectronic Engineering, 55, (2001), 5357.Google Scholar
15. Volinsky, A.A., Moody, N.R., Gerberich, W.W., Acta Mater. Vol. 50/3 441, (2002)Google Scholar
16. Antis, G.R., Chantikol, P., Lawn, B.R. and Marshall, D.B., J. of Amer. Ceram. Soc., Vol. 64, No. 9, pp. 533538, (1981)Google Scholar
17. Pharr, G.M., Harding, D.S., Oliver, W.C., Mechanical Properties and Deformation Behavior of Materials Having Ultra-Fine Microstructures, Nastasi, M. et al. (eds.), Kluwer Academic Press, pp. 449461, (1993)Google Scholar
18. Harding, D., Oliver, W., Pharr, G., MRS Symp. Proc. Vol. 356, pp. 663668, (1995)Google Scholar
19.Spectroscopic ellipsometry measurements were obtained on a commercially available JA Woollam VUV-VASE302 instrument, at three angles of incidence (65 to 75°) and from 0.7 to 9.5 eV. Cf. Edwards, N.V., Vella, J., Xie, Q., Zollner, S., Werho, D., Adhihetty, I., Liu, R., Tiwald, T.E., Russell, C., Vires, J., and Junker, K.H., Materials Research Society Symposium Proceedings, Vol. 697, P4.7 (2001)Google Scholar
20. Vella, J.B., Xie, Q., Edwards, N.V., Kulik, J., Junker, K., Materials Research Society Symposium Proceedings, Vol. 695, L6.25 (2002)Google Scholar
21. Volinsky, A.A., Vella, J.B., Gerberich, W.W., submitted to Thin Solid Films (2002)Google Scholar
22. Ostertag, C.P., Charalambides, P.C., and Evans, A.G., Acta Mater. 37(7) 2077 (1989)Google Scholar
23. Hoehn, J.W., Venkataraman, S.K., Huang, H., and Gerberich, W.W., Mat. Sci and Eng. A192/193 306 (1995)Google Scholar