Hostname: page-component-54dcc4c588-5q6g5 Total loading time: 0 Render date: 2025-10-12T07:28:16.005Z Has data issue: false hasContentIssue false

Nanoindentation Experiments on Glass and Polymers at Different Loading Rates and the Power Law Analysis

Published online by Cambridge University Press:  10 February 2011

P. Grau
Affiliation:
Department of Physics, Martin - Luther - University, Friedemann - Bach - Platz 6, 06099 Halle, Germany
H. Meinhard
Affiliation:
Department of Physics, Martin - Luther - University, Friedemann - Bach - Platz 6, 06099 Halle, Germany
S. Mosch
Affiliation:
Department of Physics, Martin - Luther - University, Friedemann - Bach - Platz 6, 06099 Halle, Germany
Get access

Abstract

Results of nanoindentation experiments on glasses and polymers, carried out at different loading rates and regimes (loading, hold segment and unloading), were compared with simulated models based on rheological principles. The best fit was obtained by combining the rheological elements for elasticity, plasticity and viscosity in series with squares of the indentation depth.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Pharr, W. C., J. Mater.Res. 7, 1564 (1992)Google Scholar
2. Grau, P., Berg, G., and Frinzel, W., Glastech.Ber.Glass Sci.Technol. 66, 313 (1993)Google Scholar
3. Tsui, T. Y., Oliver, W. C., and Pharr, G. M. Mat.Res.Symp.Proc. 436, 147 (1997)Google Scholar
4. Grau, P., Berg, G., Meinhard, H., and Mosch, S., J.Am. Ceram. Soc. (in press)Google Scholar
5. Meinhard, H., Grau, P., Berg, G., and Mosch, S., Glastech.Ber.Glass Sci.Technol. 70, 333 (1997)Google Scholar
6. Han, W.-T. and Tomozawa, M., J.Aml.CeramSoc. 73, 3626 (1990)Google Scholar
7. Meinhard, H., doctor dissertation, MLU Halle-Wittenberg, 1998 Google Scholar
8. Grau, P., Berg, G., Fränzel, W., and Meinhard, H., phys.stat.sol.(a) 146, 537 (1994)Google Scholar