Multiple-Frequency Nanoindentation Testing

Published online by Cambridge University Press:  01 February 2011

A. C. Fischer-Cripps*
Affiliation:
CSIRO Division of Industrial Physics, PO Box 218, Lindfield NSW 2070, Australia
Get access

Abstract

This paper describes a new method of dynamic nanoindentation testing whereby, instead of the imposition of a single sinusoidal modulation onto the driving force signal, a multiple-frequency modulation is applied and a Fourier analysis used to extract frequency-dependent mechanical properties. The instrument response is cancelled by the use of a reference transfer function using an equalization process. The present work gives details of the method and presents some example measurements.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7 4, 1564 (1992).Google Scholar
2. Lucas, B.N., Oliver, W.C., and Swindeman, J.E., Mat. Res. Soc. Symp. Proc. 522 3 (1998)Google Scholar
3. Doerner, M.F. and Nix, W.D., J. Mater. Res. 1 4, 601 (1986)Google Scholar
4. Burnham, N.A., Baker, S.P., and Pollock, H.M., J. Mater. Res. 15 9, 2006 (2000)Google Scholar
5. Silly Putty® is a trademark of Binney and Smith Inc, Easton, PA, USA and is manufactured by Dow Corning as 3179 Dilatent Compound.Google Scholar