Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper

Published online by Cambridge University Press:  01 February 2011

Martin Rester
Affiliation:
martin.rester@stud.unileoben.ac.at, Austrian Academy of Sciences, Erich Schmid Institute, Jahnstrasse 12, Leoben, 8700, Austria, +43 (0) 3842 / 804 - 313, +43 (0) 3842 / 804 - 116
Christian Motz
Affiliation:
christian.motz@unileoben.ac.at, Austrian Academy of Sciences, Erich Schmid Institute, Jahnstrasse 12, Leoben, 8700, Austria
Reinhard Pippan
Affiliation:
pippan@unileoben.ac.at, Austrian Academy of Sciences, Erich Schmid Institute, Jahnstrasse 12, Leoben, 8700, Austria
Get access

Abstract

The deformation zone below nanoindents in copper single crystals with an <110>{111} orientation is investigated. Using a focused ion beam (FIB) system, cross-sections through the center of the indents were fabricated and subsequently analyzed by means of electron backscatter diffraction (EBSD) technique. Additionally, cross-sectional TEM foils were prepared and examined. Due to changes in the crystal orientation around and beneath the indentations, the plastically deformed zone can be visualized and related to the measured hardness values. Furthermore, the hardness data were analyzed using the Nix-Gao model where a linear relationship was found for H2 vs. 1/hc, but with different slopes for large and shallow indentations. The measured orientation maps indicate that this behavior is presumably caused by a change in the deformation mechanism. On the basis of possible dislocation arrangements, two models are suggested and compared to the experimental findings. The model presented for large imprints is based on dislocation pile-ups similar to the Hall-Petch effect, while the model for shallow indentations uses far-reaching dislocation loops to accommodate the shape change of the imprint.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Gane, N. and Cox, J. M. Philos. Mag. 22, 881 (1970).Google Scholar
2 Pethica, J. B. Hutchings, R. and Oliver, W. C. Philos. Mag. A 48, 593 (1983).Google Scholar
3 Ma, Q. and Clark, D. R. J. Mater. Res. 10, 853 (1995).Google Scholar
4 Nix, W. D. and Gao, H., J. Mech. Phys. Solids 46, 411 (1998).Google Scholar
5 Lim, Y. Y. and Chaudhri, M. M. Philos. Mag. A 79, 2979 (1999).Google Scholar
6 Swadener, J. G. George, E. P. and Pharr, G. M. J. Mech. Phys. Solids 50, 681 (2002).Google Scholar
7 Feng, G. and Nix, W. D. Scripta Mater. 51, 599 (2004).Google Scholar
8 Oliver, W. C. and Pharr, G. M. J. Mater. Res. 7, 1564 (1992).Google Scholar
9 Rester, M., Motz, C. and Pippan, R., Acta Mater. 55, 6427 (2007).Google Scholar
10 Tabor, D., Proc. R. Soc. A 192, 247 (1947).Google Scholar
11 Hall, E. O. Proc. Phys. Soc. B 64, 747 (1951).Google Scholar
12 Petch, N. J. J. Iron Steel Inst. 174, 25 (1953).Google Scholar
13 Fisher, J. C. Hart, E. W. and Pry, R. H. Phys. Rev. 87, 958 (1952).Google Scholar
14 Friedman, L. H. and Chrzan, D. C. Philos. Mag. A 77 1185 (1998).Google Scholar
15 Blanckenhagen, B. von, Arzt, E. and Gumbsch, P., Acta Mater. 52 773 (2004).Google Scholar