Published online by Cambridge University Press: 21 March 2011
The development of a novel transmission electron microscope holder has made real time observations of nanoindentation possible. Using a piezo-ceramic loading mechanism, a diamond indenter is pushed into the surface of a sample, while the electron beam images the deforming sample in cross section. In this paper, we present the method for calibrating the force-displacement-voltage relation and load-frame compliance associated with this instrument. This allows quantitative force-displacement measurements to be obtained, in the manner of traditional indentation experiments. As an example of the utility of this technique, we present observations of the indentation behavior of an Al thin film on silicon, which have been previously shown [1]. Indentation into a coarse grain shows a displacement excursion corresponding to the nucleation of dislocations, and is compared to force-displacement responses measured with instrumented indentation techniques.