Mechanical Properties of Rapidly Solidified Nickel-Base Superalloys and Intermetallics

Published online by Cambridge University Press:  25 February 2011

A. I. Taub
Affiliation:
General Electric Corporate Research and Development, PO Box 8, Schenectady, New York 12301
M. R. Jackson
Affiliation:
General Electric Corporate Research and Development, PO Box 8, Schenectady, New York 12301
Get access

Abstract

The improvements in the mechanical properties of nickel-base alloys that have been made possible by rapid solidification processing are reviewed. The results of processing by powder metallurgy, laser melting, low pressure plasma deposition and spray forming are examined. In general, the increased homogeneity obtained by rapid solidification allows for increased alloying and improved hot workability. The refined grain size improves the low and intermediate temperature strength, but leads to lower strengths at high temperature. For the high temperature applications, post solidification grain growth is required, as for example the directional recrystallization of powder metallurgy preforms. The development of a novel means of producing a fine dispersion from amorphous alloy precursors and the recent work attempting to improve the ductility of the intermetallic phases NiAl and Ni3A1 are also described.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1986

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Cohen, M., Kear, B.H. and Mehrabian, R., “Rapid Solidificaton Processing II”, ed. Mehrabian, R., Kear, B.H. and Cohen, M., Claitors Publishing, Baton Rouge, 1980, p. 1.Google Scholar
2.Gessinger, G.H., Powder Met. Intl. 13 (1981) 93.Google Scholar
3.Tracey, V.A. and Cutler, C.P., Powder Metallurgy, 1 (1981) 32.Google Scholar
4.Gessinger, G.H., “Powder Metallurgy of Superalloys”, Butterworths Publishing, 1984, pp. 348.Google Scholar
5.Sims, C.T., “Superalloys 1984, Proceedings of Fifth Intl. Conf. on Superalloys”, ed. Gell, M., et.al., AIME, 1984, p.399.Google Scholar
6.Taub, A.I., “Rapidly Quenched Metals, Proceedings of the Fifth Intl. Conf. on Rapidly Quenched Metals”, ed. Steeb, S. and Warlimont, H., North Holland, 1985, p.1611.Google Scholar
7.Williams, J.C. and Rirth, J.P., “Rapid Solidification Processing III”, ed. Mehrabian, R., National Bureau of Standards, 1983, p.135.Google Scholar
8.Jones, H., J. Mat. Sci. 19 (1984) 1043.Google Scholar
9.Taub, A.I., Jackson, M.R., Huang, S.C. and Hall, E.L., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 28 (1984) 389.Google Scholar
10.Yasuda, K., Tsuchiyay, M., Kuroda, T. and Suwa, M., “Superalloys 1984, Proceedings of Fifth Intl. Conf. on Superalloys”, ed. Gell, M., et. al., AIME, 1984, p. 477.Google Scholar
11.Davies, H.A., Shohoji, N. and Warrington, D.H., “Rapid Solidificaton Processing II”, ed. Mehrabian, R., Kear, B.H. and Cohen, M., Claitors Publishing, Baton Rouge, 1980, p. 153.Google Scholar
12.Jackson, M.R., Rairden, J.R., Smith, J.S. and Smith, R.W., J. Metals, 33 (1981) 23.Google Scholar
13.Jackson, M.R. and Huang, S.C., “Mechanical Behavior of Rapidly Solidified Materials, Proceedings of Symposium, Feb 24-28, 1985”, AIME, in press.Google Scholar
14.Sugarman, B. and Jessop, C.T., “Symposium on Powder Metallurgy”, London, Iron and Steel Institute, 1956, p. 191.Google Scholar
15.Bourdeau, R.G. and Moore, J.B., “Rapid Solidification Processing I”, ed. Mehrabian, R., Kear, B.B. and Cohen, M., Claitors Publishing, Baton Rouge, 1978, p. 334.Google Scholar
16.Aigeltinger, E.B. and Kersker, M., Metals Forum, 4 (1981) 112.Google Scholar
17.Aigeltinger, E.H., Giamei, A.F. and Dimiduk, D.M., “Rapid Solidification Processing III”, ed. Mehrabian, R., National Bureau of Standards, 1983, p.186.Google Scholar
18.Holiday, P.R. and Patterson, R.J., “Apparatus for Producing Metal Powder”, U.S. Patent 4,078,873 (1978).Google Scholar
19.Patterson, R.J., Cox, A.R. and VanReuth, E.C., J. Metals, 39 (1980) 34.Google Scholar
20.Grant, N.J., “Rapidly Quenched Metals, Proceedings of the Fifth Intl. Conf. on Rapidly Quenched Metals”, ed. Steeb, S. and Warlimont, H., North Holland, 1985, p.1611.Google Scholar
21.Williams, B., Metal Powder Report 10 (1980) 464.Google Scholar
22.Brookes, R.G., Leatham, A.G., Dunstan, G.R. and Moore, C., “Powder Metallurgy Superalloys -Aerospace Materials for the 1980's”, Metal Powder Report, Shrewsbury, England (1980).Google Scholar
23.Evans, R.W., Leatham, A.G. and Brookes, R.G., Proc. Metals Society 1983 Powder Metallurgy Group Meeting, Metals Soc. London (1983).Google Scholar
24.Brookes, R.G., Moore, C., Leatham, A.G. and Coombes, J.S., Powder Metallurgy 2 (1977) 100.Google Scholar
25.Bricknell, R.H., “The Structure and Properties of a Nickel-Based Superalloy Produced by Osprey Atomization-Deposition”, Report No. 85CRD043, General Electric Company, Schenectady, NY (1985), also Met. Trans., in press.Google Scholar
26.Fiedler, B.C., Sawyer, T.F. and Kopp, R.W., “Spray Forming”, Report No. 85CRD073, General Electric Company, Schenectady, NY (1985).Google Scholar
27.Snow, D.B., Breinan, E.M. and Kear, B.H., “Superalloys 1980”, ed. Tien, J.K., et. al., 1980, ASM, 189.Google Scholar
28.Mordike, B.L. and Bergmann, H.W., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 28 (1984) 45.Google Scholar
29.Breinan, F.M. and Kear, B.H., “Rapid Solidification Processing I”, ed. Mehrabian, R., Kear, B.H. and Cohen, M., Claitors Publishing, Baton Rouge, 1978, p. 87.Google Scholar
30.Lin, C.J. and Spaepen, F., “Chemistry and Physics of Rapidly Solidified Materials”, ed. Berkowitz, B.J. and Scattergood, R.O., AIME, 1983, p.273.Google Scholar
31.Yunlong, G., Zhuangqi, H., Wei, G. and Changhsu, S., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 28 (1984) 99.Google Scholar
32.Strutt, P.R., LeMay, J. and Tauqir, A., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 28 (1984) 87.Google Scholar
33.Yurup, M., Tauqir, A. and Strutt, P.R., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 28 (1984) 93.Google Scholar
34.Snow, D.B., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 8 (1982) 523.Google Scholar
35.Decker, R.F. and Freeman, J.W., Trans AIME, 218 (1960) 277.Google Scholar
36.Maxwell, D.H., Baldwin, J.F. and Radavich, J.F., Metall. Met. Forming, Oct 1975, 332.Google Scholar
37.Bashev, V.F., Miroshnichonko, I.S. and Sergeev, G.A., Russ. J. Inorg. Mat., 17 (1981) 892.Google Scholar
38.Huang, S.C. and Chang, K.M., J. Mat. Sci. 19 (1984) 1220.Google Scholar
39.Giessen, B.C., Polk, D.E. and Ray, R., “High Strength Iron, Nickel and Cobalt Base Crystalline Alloys With Ultrafine Disperion of Borides and Carbides”, U.S. Patent 4,297,135, Oct. 27, 1981.Google Scholar
40.Cahn, R.W., Ann. Rev. Mater. Sci., 12 (1982) 51.Google Scholar
41.Raybould, D., Metal Powder Report, 39(1984)Google Scholar
42.Ray, R., Metal Progress, 125 (1982) 29.Google Scholar
43.Ray, R., J. Mat. Sci. Letters, 16 (1981) 2927.Google Scholar
44.Das, S.K. and Raybould, D., “Rapidly Quenched Metals, Proceedings of the Fifth Intl. Conf. on Rapidly Quenched Metals”, ed. Steeb, S. and Warlimont, H., North Holland, 1985, p.1787.Google Scholar
45.Wan, C.C., “Rapidly Solidified Amorphous and Crystalline Alloys”, Mat. Res. Soc. Symp. Proc., 8 (1982) 441.Google Scholar
46.Das, S.K., Davis, L.A., Wang, J.R.Y. and Kapoor, D., “Rapid Solidification Processing III”, ed. Mehrabian, R., National Bureau of Standards, 1983, p.559.Google Scholar
47., Anon, Metal Progress, 125 (1982) 38.Google Scholar
48.Asheley, S., Amer. Met. Market Metalworking News, 95 (1981) 14.Google Scholar
49.Anon, Metal Progress, 128 (1985) 24.Google Scholar
50.Vedula, K., Pathare, V., Aslanidis, I. and Titran, R.H., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 411.Google Scholar
51.Stephens, J.R., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 381.Google Scholar
52.Grala, E.M., “Mechanical Properties of Intermetallic Compounds”, ed. Westbrook, J.H., John Wiley, New York, 1960, 358.Google Scholar
53.Ball, A. and Smallman, R.E., Acta Met. 14 (1966) 1349.Google Scholar
54.Guard, R.W. and Westbrook, J.H., Trans TMS-AIME, 215 (1959) 807.Google Scholar
55.Noguchi, O., Oya, Y. and Suzuki, T., Met. Trans. 12A(1981)1647.Google Scholar
56.Thornton, P.E., Davies, R.G. and Johnston, T.L., Met. Trans. 1A(1970)207.Google Scholar
57.Aoki, K. and Izumi, O., J. Japan Inst. Met., 43 (1979) 1190.Google Scholar
58.Stoloff, N.S., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 3.Google Scholar
59.Taub, A.I., Huang, S.C. and Chang, K.M., Met. Trans. 15A(1984)399.Google Scholar
60.Inoue, A., Masumoto, T., Tomioka, H. and Yano, N., Int. J. of Rapid Solidification, 1 (1984) 115.Google Scholar
61.Inoue, A., Tomioka, H. and Masumoto, T., J. Mat. Sci. Letters, 1 (1982) 377.Google Scholar
62.Inoue, A., Tomioka, H. and Masumoto, T., Met. Trans. 14A(1983)1367.Google Scholar
63.Inoue, A., Tomioka, H. and Masumoto, T., J. Mat. Sci. 19 (1984) 3097.Google Scholar
64.Takasugi, T. and Izumi, O., Acts Met. 33 (1985) 1259.Google Scholar
65.Koch, C.C., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 397.Google Scholar
66.Koch, C.C., Horton, J.A., Liu, C.T., Cavin, O.B. and Scarborough, J.O., “Rapid Solidification Processing III”, ed. Mehrabian, R., National Bureau of Standards, 1983, p.26Google Scholar
67.Horton, J.A., Koch, C.C. and Liu, C.T., Proceedings 41st Annual Meeting of the Electron Microscopy Society of America, ed. Bailey, G.W., San Francisco Press (1983)248.Google Scholar
68.Schulson, F.M., Res Mech Letters 1 (1981) 111.Google Scholar
69.Schulson, E.M., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 193.Google Scholar
70.Schulson, E.M. and Baker, D.R., Scripta Met. 17 (1983) 519.Google Scholar
71.Gaydosh, D.J., Jech, R.W. and Titran, R.H., J. Mat. Sci. Letters 4 (1985) 138.Google Scholar
72.Gaydosh, D.J. and Crimp, M.A., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 429.Google Scholar
73.Aoki, K. and Izumi, O., J. Mat. Sci., 14 (1979) 1800.Google Scholar
74.Takasugi, T., George, E.P., Pope, D.P. and Izumi, O., Scripts Met 19 (1985) 551.Google Scholar
75.Ogura, T., Hanada, S., Masumoto, T. and Izumi, O., Met Trans 16A(1985)441.Google Scholar
76.Liu, C.T., White, C.L. and Horton, J.A., Acta. Met. 33 (1985) 213.Google Scholar
77.Huang, S.C., Taub, A.I., Chang, K.-M., Briant, C.L. and Hall, E.L., 403Proceedings of the Fifth International Conference on Rapidly Quenched Metals, Wurzburg, Germany, Sept. 1984”, ed. Steeb, S. and Warlimont, H., North Holland, Amsterdam (1985)1407.Google Scholar
78.Liu, C.T., White, C.L., Koch, C.C. and Lee, E.H., Proceedings of the Electrochemical Society on High Temperature Materials, ed. Cubic-ciotti, Munir, Vol. 83–87, Electrochemical Society Inc. (1983), p. 32.Google Scholar
79.Messmer, R.P. and Briant, C.L., Acta Met 30 (1982) 457.Google Scholar
80.Liu, C.T. and White, C.L., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 365.Google Scholar
81.Huang, S.C., Taub, A.I. and Chang, K.M., Acta Met. 32 (1984) 1703.Google Scholar
82.Chang, K.M., Taub, A.I. and Huang, S.C., “High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 335.Google Scholar
83.Taub, A.I., Huang, S.C. and Chang, K.M., “Failure Mechanisms in High Performance Materials, Proc. 39th Meeting of Mechanical Failures Prevention Group”, ed. Early, J.G., Shives, T.R. and Smith, J.H., Cambridge University Press (1985)57.Google Scholar
84.Lopez, J.A. and Hancock, G.F., Phys. Stat. Sol. A 2 (1970) 469.Google Scholar
85.Rawlings, R.D. and Staton-Bevan, A.E., J. Mat. Sci. 10 (1975) 657.Google Scholar
86.Taub, A.I., Huang, S.C. and Chang, K.M.High Temperature Ordered Intermetallic Alloys”, Mat. Res. Soc. Symp. Proc., 39 (1985) 221.Google Scholar
87.Liu, C.T., White, C.L. and Lee, E.H., Scripta Met, in press.Google Scholar
88.Liu, C.T. and White, C.L., Acta Met., in press.Google Scholar
89.Taub, A.I., Briant, C.L., Huang, S.C., Chang, K.M. and Jackson, M.R., Scripta Met., in press.Google Scholar
90.Takasugi, T. and Izumi, O., Acta Met. 33 (1985) 1247.Google Scholar