Investigation of Mechanical Properties of CrN-PVD Thin Films by Nanoindentation

Published online by Cambridge University Press:  10 February 2011

E. Lugscheider
Affiliation:
Aachen University of Technology, Materials Science Institute, 52056 Aachen, Germany
O. Knotek
Affiliation:
Aachen University of Technology, Materials Science Institute, 52056 Aachen, Germany
C. Barimani
Affiliation:
Aachen University of Technology, Materials Science Institute, 52056 Aachen, Germany
S. Guerreiro
Affiliation:
Aachen University of Technology, Materials Science Institute, 52056 Aachen, Germany
M. Lake
Affiliation:
Aachen University of Technology, Materials Science Institute, 52056 Aachen, Germany
Get access

Abstract

The hardness of PVD thin films is of great interests regarding to their applications. It is well known that the hardness is influenced by different deposition energies. For the present work, two different coating processes were used to deposit a CrN layer on high speed steels type HS 6-5-2 (M2). The deposition processes were carried out by the Cathodic Arc Ion Plating Process (AIP) and the Magnetron Sputter Ion Plating Process (MSIP) by varying the deposition energy. The AIP process was used to deposit coatings under a strong ion bombardment. Magnetron Sputtering was used for comparison with the AIP process. The MSIP process is distinguished by a lower emission of ions in contrast to the AIP process.

To evaluate the film hardness of CrN PVD coatings the NanoindenterTM XP was used taking into account the different deposition energies and ionization levels as characteristics of the used deposition processes. A strong chromium ion bombardment leads to a homogenous and uniform coatings structure. As shown in this paper, the film hardness is mainly influenced by the coatings microstructure generated by different deposition energies.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Thornton, J.A., Ann. Rev. Mater. Sci. 7, (1997), p. 239260.Google Scholar
2 Messier, R., Giri, A.P. and Roy, R.A., J. Vac. Sci. Technol., A2 (2), April-June 1984.Google Scholar
3 Rickerby, D.S. and Bull, S.J., Surf. Coat. Technol. 39/40, (1990), p. 315.Google Scholar
4 Johnson, P.C., in Vossen, J.L. and Kern, W. (eds.), Thin Films Processes II, Ch. II5, p. 209.Google Scholar
5 Scholl, H.J., Doct. Thesis, Aachen University of Technology, Verlag Mainz, Aachen, 1993.Google Scholar
6 Lugscheider, E., Barimani, C., Wolff, C., Guerreiro, S. and Döpper, G., Surf. Coat. Technol., 86–87 (1996), p. 177183.Google Scholar
7 Bueckle, H. in VDI-Berichte Nr. 160, edited by VDI-Verlag, , Duesseldorf, , 1972, p. 524.Google Scholar
8 Doemer, M.F. and Nix, W.D., J. Mater. Res. 1 (1986), p. 601609.Google Scholar
9 Page, T.F. and Hainsworth, S.V., Surf. Coat. Technol., 61 (1993), p. 201208.Google Scholar
10 Hainsworth, S.V. and Page, T.F., Surf. Coat. Technol., 68–69 (1994), p. 571575.Google Scholar
11 Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, (1992), p. 15641583.Google Scholar
12 Gautier, C., Moussaoui, H., Elstner, F. and Machet, J., Surf. Coat. Technol., 86–87 (1996), p. 254262.Google Scholar
13 Grant, W.K., Loomis, C., Moore, J.J., Olson, D.L., Mishra, B. and Perry, A.J., Surf. Coat. Technol., 86–87 (1996), p. 788796.Google Scholar