Hostname: page-component-54dcc4c588-smtgx Total loading time: 0 Render date: 2025-10-13T13:45:13.922Z Has data issue: false hasContentIssue false

Internal Strains Of A Creep Deformed Single Crystal Nickel-Based Superalloy

Published online by Cambridge University Press:  22 February 2011

Uwe Glatzel
Affiliation:
Mikrostrukturanalyse, Sekr. BH 18, Technische Universität Berlin, D-10623 Berlin, Germany
Andreas MÜller
Affiliation:
Strukturforschung, Hahn-Meitner-Institut, Glienickerstr. 100, D-14109 Berlin, Germany
Get access

Abstract

Neutron scattering experiments have been carried out with undeformed and creep deformed samples of the superalloy CMSX-4. From the measured constrained misfit data, obtained from different reflecting planes with respect to the external load axis, two strain tensors for horizontal and vertical matrix plates can be extracted.

A careful data analysis is necessary since the technical manufactured single crystals show a mosaic spreading of 0.5° and the wavelength spreading of the incident neutron beam, Δλ/λ is about 410-3 This is in the same range as the unknown constrained misfit quantities δc. A method has been developed which allows a calculated intensity distribution to be fitted to the measured one.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1 Frazier, D.J., Whetstone, J.R., Harris, K., Erickson, G.L. and R.E, Schwer, High Temperature Materials for Power Engineering, Cost 501/505 Conf., Liège (1990)Google Scholar
2 Glatzel, U., Microstructure and Internal Strains of Undeformed and Creep Deformed Samples of a Nickel-Base Superalloy (Verlag Köster, Berlin, 1994), ISBN 3-929937-91-3Google Scholar
3 Glatzel, U. and Müller, A., Scripta Met. Mat. 31, 285 (1994)Google Scholar
4. Glatzel, U., Scripta Met. Mat. 31, 291 (1994)Google Scholar
5 Glatzel, U. and Müller, A., Numerical Predictions of Deformation Processes and the Behaviour of Real Materials, edited by Andersen, S.I. et al. , (Riso National Laboratory, Roskilde, Denmark, 1994), 319 Google Scholar
6 Müller, L., Glatzel, U. and Feller-Kniepmeier, M., Acta Met. Mat. 41, 3401 (1993)Google Scholar
7 Schmidt, R. and Feller-Kniepmeier, M., Scripta Met. Mat. 29, 1079 (1993)Google Scholar