In-situ electrical probing of zones of nanoindentation-induced phases of silicon

Published online by Cambridge University Press:  01 February 2011

Simon Ruffell
Affiliation:
simon.ruffell@anu.edu.au, Australian National University, Electronic Materials Engineering, Canberra, Australian Capital Territory, Australia
Jodie Bradby
Affiliation:
jodie.bradby@anu.edu.au, Australian National University, Electronic Materials Engineering, Canberra, Australian Capital Territory, Australia
Jim Williams
Affiliation:
jsw109@rsphysse.anu.edu.au, Australian National University, Electronic Materials Engineering, Canberra, Australian Capital Territory, Australia
Ryan Major
Affiliation:
rmajor@hysitron.com, Hysitron Inc., Minneapolis, Minnesota, United States
Oden Warren
Affiliation:
owarren@hysitron.com, Hysitron Inc., Minneapolis, Minnesota, United States
Get access

Abstract

Phase transformed zones of silicon have been formed by nanoindentation both at the micro- and nanoscale and electrically probed using an in-situ measurement system. Zones composed of the high pressure crystalline phases (Si-III/Si-XII) have higher conductivity than those of amorphous silicon (a-Si). At the microscale probing laterally across the surface shows that the conductivity varies within the zones composed of the high pressure phases. The sensitivity to the different conductivities of the two phases allows mapping within the zones. Finally, at the nanoscale the conductivity of the high pressure phase zones can be correlated with the position of the pop-out associated with the formation of the phases. The zones have higher conductivity when the pop-out occurs earlier on unloading and we suggest that this is due to the reduction in trace volumes of a-Si formed during the early portion of the unloading cycle.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Bradby, J. E., Williams, J. S., Wong-Leung, J., Swain, M. V. and Munroe, P., Journal of Materials Research, 16: p. 1500 (2001).Google Scholar
2. Domnich, V. and Gogotsi, Y., Reviews on Advanced Materials Science, 3: p. 136 (2002).Google Scholar
3. Kailer, A., Gogotsi, Y. G. and Nickel, K. G., Journal of Applied Physics, 81: p. 3057 (1997).Google Scholar
4. Pharr, G. M., Oliver, W. C. and Harding, D. S., Journal of Materials Research, 6: p. 1129 (1991).Google Scholar
5. Ruffell, S., Bradby, J. E. and Williams, J. S., Applied Physics Letters, 89(9): p. 091919 (2006).Google Scholar
6. Williams, J.S., Chen, Y., Wong-Leung, J., Kerr, A. and Swain, M.V., Journal of Materials Research, 14: p. 2338 (1999).Google Scholar
7. Zarudi, I., Zhang, L. C., Zou, J. and Vodenitcharova, T., Journal of Materials Research, 19: p. 332 (2004).Google Scholar
8. Mann, A. B., van Heerden, D., Pethica, J. B., Bowes, P. and Weihs, T. P., Philosophical Magazine A, 82(10): p. 1921 (2002).Google Scholar
9. Ruffell, S., Bradby, J. E., Fujisawa, N. and Williams, J. S., Journal of Applied Physics, 101: p. 083531 (2007).Google Scholar
10. Ruffell, S., Bradby, J. E., Williams, J. S. and Warren, O. L., Journal of Materials Research, 22(3): p. 578 (2007).Google Scholar
11. Beeson, J. M., Mokhtari, E. H., Gonzalez, J. and Weill, G., Physical Review Letters, 59(4): p. 473 (1987).Google Scholar
12. Malone, B. D., Sau, J. D. and Cohen, M. L., Physical Review B, 78: p. 035210 (2008).Google Scholar
13. Ruffell, S., Bradby, J. E. and Williams, J. S., (unpublished).Google Scholar
14. Ruffell, S., Bradby, J. E., Williams, J. S. and Munroe, P., Journal of Applied Physics, 102: p. 063521 (2007).Google Scholar