In situ Neutron Diffraction Studies of Carbide-Matrix Interactions in HAYNES® 230® Nickel Based Superalloy

Published online by Cambridge University Press:  01 February 2011

Tarik A. Saleh
Affiliation:
Department of Materials Science and Engineering, University of Tennessee, Knoxville, TN 37996, U.S.A. Los Alamos Neutron Science Center, Los Alamos National Laboratory, Los Alamos, NM 87545, U.S.A.
Bjørn Clausen
Affiliation:
Los Alamos Neutron Science Center, Los Alamos National Laboratory, Los Alamos, NM 87545, U.S.A.
Donald W. Brown
Affiliation:
Los Alamos Neutron Science Center, Los Alamos National Laboratory, Los Alamos, NM 87545, U.S.A.
Hahn Choo
Affiliation:
Department of Materials Science and Engineering, University of Tennessee, Knoxville, TN 37996, U.S.A. Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831, U.S.A.
Peter K. Liaw
Affiliation:
Department of Materials Science and Engineering, University of Tennessee, Knoxville, TN 37996, U.S.A.
Mark A. M. Bourke
Affiliation:
Los Alamos Neutron Science Center, Los Alamos National Laboratory, Los Alamos, NM 87545, U.S.A.
Sven C. Vogel
Affiliation:
Los Alamos Neutron Science Center, Los Alamos National Laboratory, Los Alamos, NM 87545, U.S.A.
Raymond A. Buchanan
Affiliation:
Department of Materials Science and Engineering, University of Tennessee, Knoxville, TN 37996, U.S.A.
Dwaine L. Klarstrom
Affiliation:
Haynes International, Inc., Kokomo, IN 46904, U.S.A.
Get access

Abstract

HAYNES 230 is a solid solution strengthened, face centered cubic (FCC), nickelbased superalloy, with a small amount (1–5 vol. %) of semi-coherent FCC carbides. Neutron diffraction experiments were performed to study the interaction of the carbides with the matrix during tensile and compressive loading. The behavior of the elastic lattice strains during in situ loading clearly showed a tension-compression asymmetry. Although the volume percentage is small, the interaction between the carbides and the matrix had a significant effect on the load sharing. In compression, the carbides began load sharing at the macroscopic yield point, while the tension test suggests no load sharing. Debonding at the carbide-matrix interface is proposed to explain the lack of load sharing during the tensile loading based on the disparities observed between the experimental results and the finite element models.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. HAYNES 230 Alloy Product Brochure, H-3000, Haynes International. www.haynesint.com Google Scholar
2. Daymond, M. R., Bourke, M. A. M., Von Dreele, R. B., Clausen, B. and Lorentzen, T., J. Appl. Phys. 82, 4, (1997).Google Scholar
3. Bourke, M. A. M., Dunand, D.C., and Ustundag, E., Appl. Phys. A 74, S1707–S1709 (2002).Google Scholar
4. Stone, H. J., Holden, T. M., and Reed, C. R., Acta Mater. 47 (17), 44354448 (1999).Google Scholar
5. Choo, H., Bourke, M. A. M., Nash, P., Daymond, M., Shi, N., Mat. Sci. & Eng, A. 264, 108121 (1999).Google Scholar
6. ASTM Standard E 8–04, Standard Test Methods for Tension Testing Metallic Materials 6.Google Scholar
7. Larson, A.C. and Von Dreele, R.B., Los Alamos National Laboratory Report LAUR 86748 (2000).Google Scholar
8. ABAQUS User Manual, version 6.3, Hibbitt, Karlsson and Sorensen, Inc., (2002) www.abaqus.com.Google Scholar
9. Clausen, B., Lee, S.-Y., Üstündag, E., Aydiner, C.C., Conner, R.D., Bourke, M.A.M., Scripta Materalia 49 (2), 123128, (2003).Google Scholar
10. Allen, A. J., Bourke, M. A. M., Dawes, S., Hutchings, M. T., Withers, P. J., Acta Metallurgica et Materialia 40 (9), 2361–73 (1992).Google Scholar
11. Povirk, G. L., Stout, M. G., Bourke, M., Goldstone, J. A., Lawson, A. C., Lovato, M., Macewen, S. R., Nutt, S. R., Needleman, A., Acta Metallurgica et Materialia 40 (9), 2391–412 (1992)Google Scholar
12. Withers, P. J., Clarke, A. P., Acta Materialia 46 (18), 6585–98 (1998).Google Scholar