Improvement of Barrier Properties of TaN Film by Plasma Enhanced Atomic Layer Deposition

Published online by Cambridge University Press:  01 February 2011

In Cheol Baek
Affiliation:
icbaek@dsemi.com, Dongbu Electronics, Advanced Nano-tech Development Division, 474-1, Sangwoo-Ri, Gamgok-Myeon, Eumseong-Gun, Chungbuk, 369-852, Korea, Republic of, +82-43-879-5860, +82-43-879-9911
Han Choon Lee
Affiliation:
chuny20@dsemi.com, Dongbu Electronics, Advanced Nano-tech Development Division, 474-1 Sangwoo-ri, Gamgok-myeon, Eumseong-gun, Chungbuk, 369-852, Korea, Republic of
Cheonman Sim
Affiliation:
shimnamwoo@dsemi.com, Dongbu Electronics, Advanced Nano-tech Development Division, 474-1 Sangwoo-ri, Gamgok-myeon, Eumseong-gun, Chungbuk, 369-852, Korea, Republic of
Jae Won Han
Affiliation:
hanjw@dsemi.com, Dongbu Electronics, Advanced Nano-tech Development Division, 474-1 Sangwoo-ri, Gamgok-myeon, Eumseong-gun, Chungbuk, 369-852, Korea, Republic of
Kee Ho Kim
Affiliation:
keehokim@dsemi.com, Dongbu Electronics, Advanced Nano-tech Development Division, 474-1 Sangwoo-ri, Gamgok-myeon, Eumseong-gun, Chungbuk, 369-852, Korea, Republic of
Soo Hyun Kim
Affiliation:
shkim@isp-tech.com, IPS Ltd., Advanced Development Team, 33, Jije-dong, Pyeongtaek, Gyeonggi-do, 450-090, Korea, Republic of
Sahng Kyoo Lee
Affiliation:
sklee@ips-tech.com, IPS Ltd., Advanced Development Team, 33, Jije-dong, Pyeongtaek, Gyeonggi-do, 450-090, Korea, Republic of
Get access

Abstract

The barrier metal properties of Plasma Enhanced ALD (PEALD) TaN deposited on low-k dielectric film (SiCOH) with a k value of 3.0 at a deposition temperature of 300°C by using pentakis (ethylmethylamino) tantalum (PEMAT) and various plasma gases was investigated. The film resistivity of TaN is about 1000 μΩ.cm under the plasma power of 200 W and the frequency of 400 KHz, respectively. The resistivity was significantly reduced by approximately 360 μΩ.cm for the optimized condition of 300 W and 13.56 MHz. In addition, good uniformity was obtained by applying two-step plasma treatment process. The film thickness per cycl of the TaN using two-step plasma was decreased from 1.0 Å to 0.65 Å by reducing a base pressure, indicating the increase of the film density. The PEALD TaN with almost 100% coverage in this paper's dual damascene structure has a contact resistance of about 1.6 Ω /chain at via size of 0.19um.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

references

1 Min, J. S., Park, H. S., and Kang, S. W., Appl. Phys. Lett., 75, 1521 (1999).Google Scholar
2 Jeon, H., Lee, J. W., Kim, Y. K., Kim, D. S. and Yi, K. S., J. Vac. Sci. & technol. 18, 1595 (2000).Google Scholar
3 Lee, J., Koo, J., Sim, H., Won, Y. and Jeon, H., J. Korean. Phys. Soc. 44, 915 (2004).Google Scholar
4 Yokoyama, N., Hinode, K., and Homma, Y., J. Electrochem. Soc., 136, 882 (1989).Google Scholar
5 Min, J. S., Park, J. S., Park, H. S., and Kang, S. W., J. Electrochem. Soc., 147, 3836 (2000).Google Scholar
6 Park, J., Park, H. and Kang, S. W., J. Electrochem. Soc. 149, C28 (2002).Google Scholar
7 Kim, J., Lee, K., Park, H., Kim, Y., and Jeon, H., J. Korean. Phys. Soc. 45, 1069 (2004).Google Scholar