Fractographic Observation of Fatigue Crack Growth in Cast Ni3Al-Based Alloys

Published online by Cambridge University Press:  26 February 2011

Yin Wanquan
Affiliation:
Institute of Metal Research, Academia Sinica 72 Wenhua Road, Shenyang 110015, P.R. China
Gao Wei
Affiliation:
Institute of Metal Research, Academia Sinica 72 Wenhua Road, Shenyang 110015, P.R. China
Zhu Yaoxiao
Affiliation:
Institute of Metal Research, Academia Sinica 72 Wenhua Road, Shenyang 110015, P.R. China
Get access

Extract

Fatigue behaviour of cast Ni3Al-based alloys with the addition of alloying elements, such as Hf, Zr and Ti etc., has been investigated. It was found that: (1) The alloying elements change remarkably mechanical property and fatigue property of cast Ni3Al-based alloys, in which, the fatigue strenghts of No.1 and No.2 alloys are 215.6MPa and 205.8MPa respectively, while that of No.3 alloy is only 78MPa, for the same cyclic life of 107; (2) Fatigue cracks initiate at the (γ'+γ) /γ interface and “matrix channel” in No.1 and No.2 alloys are at the grain-boundary or micropore, of No.3 alloy often fatigue cracks initiated from the edge of specimen under the cyclic stress; (3) Fbitigue crack propagation of cast Ni3Al-based alloys follows “zigzag” propagation path, and it proceeds through the big blocky (γ'+γ) eutectic and “matrix channel” and along the (γ';+γ)/γ interface in No.1 and No.2 alloys, while the fatigue crack propagation of No.3 alloy sometimes follows the “zigzag” propagation path. Finally, the effect of alloying elements on the fatigue behaviour of cast Ni3Al-based alloys has been discussed.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Liu, C.T. et al. . Acta Metall. 35, No.3,(1987) 643649.CrossRefGoogle Scholar
2. Ogura, T. et al. . Metall. Trans. A. 16A (1985) 441443.Google Scholar
3. Taub, A.I. et al. . Metall. Trans. A, 15A (1984) 399.Google Scholar
4. Yizhang, Zho et al. . Mat. Res. Soc. Symp. Proc.Vol 133 (1989 Materials Research Society) 555559.Google Scholar
5. Fuchs, G.E. et al. . Mat. Res. Soc. Symp. Proc. Vo181(1987 Materials Research sociely), 247261.Google Scholar