Hostname: page-component-54dcc4c588-5q6g5 Total loading time: 0 Render date: 2025-10-09T15:24:06.426Z Has data issue: false hasContentIssue false

ETCH Rate and Thickness Measurements of Layered GaAs, AlAs and AlGaAs Structures Using a Laser Reflectance Technique

Published online by Cambridge University Press:  22 February 2011

Louise H. Grober
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ. 07974
M. Hong
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ. 07974
R.D. Grober
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ. 07974
J.P. Mannaerts
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ. 07974
R.S. Freund
Affiliation:
AT&T Bell Laboratories, Murray Hill, NJ. 07974
Get access

Abstract

Laser reflectometry has been shown to be a useful tool for etch depth measurements during etching of multiple layer structures. We have extended the use of laser reflectometry to accurately determine the etch rates of GaAs, Al0.4Ga0.6As and AlAs as a function of temperature and to verify layer thickness in-situ. By use of computer simulation we compare a theoretical model to actual data to determine layer thicknesses and accurate etch rates. We compare our data to previously published work for GaAs etching.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1 Hayes, T.R., Heimann, P.A., Donnelly, V.M. and Strege, K.E., Appl. Phys. Lett. 57, 2817 (1990).Google Scholar
2 Busta, H.H., Proc. Soc. Photo-Opt. Instrum. Eng. 276, 164 (1981).Google Scholar
3 , Hecht and , Zajac, Optics, (Addison Wesley, New York, 1979), pg. 311.Google Scholar
4 Yao, y., Snyder, P.G. and Woollam, J.A., J. Appl., Phys. 70, 3261 (1991).Google Scholar
5 Aspnes, D.E., Kelso, S.M., Logan, R.A. and Bhat, R., J. Appl., Phys. 60, 754 (1986).Google Scholar
6 Ludviksson, A., Xu, M. and Martin, R. M., Surface Science 277, 282300 (1992).Google Scholar
7 Furuhata, N., Miyamoto, H., Okamoto, A. and Ohata, K., J. Appl. Phys. 65, 168 (1989).Google Scholar
8 Balooch, M., Olander, D.R. and Siekhaus, W.J., J. Vac. Sci. Technol. B 4, 794 (1986).Google Scholar
9 French, C.L, Balch, W.S. and Foord, J.S., J Phys.: Condens. Matter 3, S351–S355 (1991).Google Scholar
10 Lee, H.G., Fisher, R.J., Zydzik, G.J. and Cho, A.Y., J. Vac. Sci. Technol. B 11, 989 (1993)Google Scholar