Hostname: page-component-84c44f86f4-4zjdz Total loading time: 0 Render date: 2025-10-14T19:47:05.139Z Has data issue: false hasContentIssue false

Estimation of Firing Temperature and Compositional Variability of Archaeological Pottery by Differential Scanning Calorimetry

Published online by Cambridge University Press:  01 February 2011

A. Giordana
Affiliation:
Diagnostic Instrumentation and Analysis Laboratory (DIAL) at Mississippi State University, 205 Research Blvd., Starkville, MS 39759
E. Peacock
Affiliation:
Cobb Institute of Archaeology at Mississippi State University (MSU), P.O. Box AR, Mississippi State, MS 39762
M. McCarthy
Affiliation:
Diagnostic Instrumentation and Analysis Laboratory (DIAL) at Mississippi State University, 205 Research Blvd., Starkville, MS 39759
K. Guilbeau
Affiliation:
Now at the College of Veterinary Medicine of MSU, Starkville, MS 39759
P. Jacobs
Affiliation:
Cobb Institute of Archaeology at Mississippi State University (MSU), P.O. Box AR, Mississippi State, MS 39762
J.D. Seger
Affiliation:
Cobb Institute of Archaeology at Mississippi State University (MSU), P.O. Box AR, Mississippi State, MS 39762
W.G. Ramsey
Affiliation:
Now at Earthstone, LTD, 555 Republic Dr. Ste 440, Plano, TX 75074.
Get access

Abstract

Digital Scanning Calorimetry (DSC), a thermal characterization technique, can be used to rapidly obtain a rough upper estimate of the firing temperature of archaeological pottery as well as an indication of its composition. The technique involves heating a small sample (10–20 mg) of ground ceramic above the vitrification temperature, cooling and reheating. The curves of the two heating cycles are then compared. The validity of the technique was evaluated by a blind test in which 35 tiles fired at different temperatures were analyzed without knowing their firing point, and by analysis of archaeological pottery samples assumed to be local or imported based upon stylistic criteria.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1 Kennett, D.J., Sakai, S., Neff, H., Gossett, R., and Larson, D.O., Journal of Archaeological Science (2002) 29, 443445.Google Scholar
2 Cogswell, J.W., Neff, H., and Glascock, M.D.., Journal of Archaeological Science (1996) 23, 283287.Google Scholar
3 Hall, M.E., Brimmer, S.P., Li, F.H., and Yablonsky, L., Journal of Archaeological Science (1998) 25, 545552.Google Scholar
4 Lawrence, W.G. and West, R.R., Ceramic Science for the Potter, First Edition, Chilton Books, Philadelphia, PA, 1972, p. 54.Google Scholar
5 In this paper the word “clay” is used to indicate the material, as collected from a quarry, that is going to be used from the potter to form his wares.Google Scholar
7 Hoard, R.J., O'Brien, M.J., Khorasgany, M.G., and Gopalaratnam, V.S., Journal of Archaeological Science (1995) 22, 823832.Google Scholar