Effect of Film Thickness on the Nanoindentation Measurements of Hard Diamondlike Carbon Films Prepared by Pulsed Laser Deposition

Published online by Cambridge University Press:  17 March 2011

Q. Wei
Affiliation:
NSF Center for Advanced Materials and Smart Structures, Department of Mechanical Engineering, North Carolina A&T State University, Greensboro, NC 27411
J. Sankar
Affiliation:
NSF Center for Advanced Materials and Smart Structures, Department of Mechanical Engineering, North Carolina A&T State University, Greensboro, NC 27411
A. K. Sharma
Affiliation:
Department of Materials Science and Engineering, Burlington Labs, P. O. Box 7916, North Carolina State University, Raleigh, NC 27695-7916
J. Narayan
Affiliation:
Department of Materials Science and Engineering, Burlington Labs, P. O. Box 7916, North Carolina State University, Raleigh, NC 27695-7916
Get access

Abstract

We have investigated the effect of film thickness on the nanoindentation measurements of hard diamondlike carbon (DLC) films. The DLC films were deposited on Si (100) substrates by pulsed excimer laser deposition (KrF, λ=248nm, duration=25 ns, energy density about 3.0 J/cm2, repetition rate 10 Hz) in high vacuum (∼5×10−7torr) at room temperature for various periods of time (from 5 minutes to 20 minutes). The thickness of the films was measured by optical profilometry, and ranges from 200 to 50 nm. The nanohardness and elastic modulus of these films were measured by a depth-sensing nanoindentation technique with NanoindenterXP. Preliminary experimental observations show that the nanoindentation results are a function of film thickness. Both the hardness and Young's modulus versus displacement curves of the 200nm thick film exhibit a peak at around tenth of the film thickness. The rest of the samples with smaller film thickness show plateaus, which are higher than the hardness and Young's modulus values of the substrate.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. 1. Spear, K. E., J. Am. Ceram. Soc. 72, 171 (1989).Google Scholar
2. Friedmann, T. A., Sullivan, J. P., Knapp, J. A., Tallant, D. R., Follstaedt, D. M., Medlin, D. L. and Mirkarimi, P. B., Appl. Phys. Lett. 71, 3820 (1997).Google Scholar
3. Robertson, J., Prog. Solid State Chem. 21, 199 (1991).Google Scholar
4. Milne, W. I., J. Non-cryst. Solids 198–200, 605 (1996).Google Scholar
5. Krishnaswamy, J., Rengan, A., Narayan, J., Vedam, K. and McHargue, C. J., Appl. Phys. Lett. 54, 2455 (1989).Google Scholar
6. McKenzie, D. R., D. Muller, A. and Pailthorpe, B. A., Phys. Rev. Lett. 67, 773 (1991).Google Scholar
7. Cuomo, J. J., Doyle, J. P., Bruley, J. and Liu, J. C., Appl. Phys. Lett. 58, 466 (1991).Google Scholar
8. Cuomo, J. J., Doyle, J. P., Bruley, J. and Liu, J. C., J. Vac. Sci. Technol. A9, 2210 (1991).Google Scholar
9. Akkerman, Z. L., Efstathiadis, H. and Smith, F. W., J. Appl. Phys. 80, 3068 (1996).Google Scholar
10. Savvides, N. and Bell, T. J., J. Appl. Phys. 72, 2791 (1992).Google Scholar
11. Kulik, J., Lifshitz, Y., Lempert, G. D., Rabalais, J. W. and Marton, D., J. Appl. Phys. 76, 5063 (1994).Google Scholar
12. Chhowalla, M., Yin, Y., Amaratunga, G. A. J., McKenzie, D. R. and Frauenheim, Th.. Diamond Relat. Mater. 6, 207 (1997).Google Scholar
13. Papas, D. L., Saenger, K. L., Bruley, J., Krakow, W., Cuomo, J. J., Gu, T. and Collins, R. W., J. Appl. Phys. 71, 5675 (1992).Google Scholar
14. Bentzon, M. O., Mogensen, K., Hansen, J. B., Hansen, B. B., Taholt, C., Holiday, P. and Eskildsen, S. S., Surf. Coat. Technol., 68–69, 651655 (1994).Google Scholar
15. Wei, Q., Narayan, R. J., Sharma, A. K., Sankar, J. and Narayan, J., J. Vac. Sci. Technol. A17 (6), 34063414 (1999).Google Scholar
16. Wei, Q., Narayan, R. J., Narayan, J., Sankar, J. and Sharma, A. K., Mater. Sci. Eng., B53, 52 (1998).Google Scholar
17. Tsui, T. Y. and Pharr, G. M., J. Mater. Res. 14, 292 (1999).Google Scholar
18. Lifshitz, Y., Kasi, S. R. and Rabalasi, J. W., Mater. Sci. Forum, 52–53, 237 (1989).Google Scholar