A Differential Scanning Calorimetry (DSC) Study on The Pyrolysis Mechanism of Zinc Oxide CVD Precursor, Zinc Acetylacetonate

Published online by Cambridge University Press:  11 February 2011

Yuneng Chang
Affiliation:
Lunghwa University of Science and Technology, Dept. of Chemical Engineering, No.300, Sec.1, Wanshow Rd., Gueishan, Taoyuan, 333, Taiwan, R.O.C.
Junhsuan Hsieh
Affiliation:
Lunghwa University of Science and Technology, Dept. of Chemical Engineering, No.300, Sec.1, Wanshow Rd., Gueishan, Taoyuan, 333, Taiwan, R.O.C.
Chonan Wang
Affiliation:
Lunghwa University of Science and Technology, Dept. of Chemical Engineering, No.300, Sec.1, Wanshow Rd., Gueishan, Taoyuan, 333, Taiwan, R.O.C.
Liting Hong
Affiliation:
Lunghwa University of Science and Technology, Dept. of Chemical Engineering, No.300, Sec.1, Wanshow Rd., Gueishan, Taoyuan, 333, Taiwan, R.O.C.
Get access

Abstract

In this study, we used differential scanning calorimetry (DSC) to study pyrolysis kinetics of zinc acetylacetonate (Zn(acac)2) in chamber ambient simulating real CVD condition, with heating rate from 10 to 20 °C/min. For Zn(acac)2 heated in pure N2, inert environment, DSC showed three endothermic peaks locating at 91–106 °C, 121–128 °C, and 135–142 °C, with peak area being 88 KJ/mol, 14 KJ/mol, and 18 KJ/mol, respectively. The DSC residuals analyzed by IR indicated all peaks might be originated from physical phenomena, since no compositional change observed. Further study by temperature programmed polarized optical microscope (POM) showed these peaks might be related to dehydration, phase transition, and melting of Zn(acac)2 and its hydrates. DSC in oxygen-containing ambient with O2 concentration from to 13 to 40 % showed three endothermic peaks and two additional exothermic broad peaks at higher temperature, 209–236 °C, and 330–400 °C. These exothermic peaks are assigned to oxidative decomposition of Zn(acac)2 and releasing of ligands. When oxygen concentration increased, peak area grew. Positions of these peaks depend on heating rate. Increasing the heating rate caused every peak to shift toward higher temperatures, with the first two endothermic peaks merged into one broad one.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Chang, Yuneng, Lu, Hengchuan, Hung, Yumeng, and Lee, Chunsung, Qiu, Junquan, Li, Xinji, Zhan, Yixuan, this symposium (2002).Google Scholar
2. Berg, E.G., and Truemper, J.T., J. Phys. Chem., 64, 487 (1960).Google Scholar
3. Beech, G., Thermochimica Acta, 3, 97 (1971).Google Scholar
4. Glavas, M.J., Glasnik Hemijskog Drustva, 32, No 2–4, 229(1967).Google Scholar
5. Patnaik, M., J. Radiational Nucl. Chem. Letters, 128/4/, 283 (1988).Google Scholar
6. Miller, B.J.A., Self, V.A., Chapman, S.M., and Sermon, P.A., J. Mater. Chem., 7(10), 2155 (1997).Google Scholar
7. Puchert, M.K., Lamb, R.N., and Martin, J.W., J. Mater. Res., 11, no. 10, 2463 (1996).Google Scholar
8. Frenkel, J., Z. Phys., 35, 652 (1926),Google Scholar
b) Wagner, C., Schottky, W., Z. Phys. Chem., Abt. B11, 163 (1930).Google Scholar
c) Henisch, H.K., Rectifying Semiconductor Contacts (Oxford University Press, London, 1957), pp. 8894.Google Scholar
9. Tanaka, T., Ibaraka, T., and Fujinaka, M., Thin Sold Films, 189, 9 (1990).Google Scholar
10. Savage, J.A. and Dodsom, E.M., J. Mater. Science 4, 809 (1969).Google Scholar
11. Labau, M, Rey, P., and Delabouglise, G., Thin Sold Films, 213, 94 (1992).Google Scholar
12. Chang, Yuneng, “Organometallic Chemical vapor deposition of copper oxide thin films”, p. 75, Ph.D. Thesis, Iowa Sate Univ., Ames, IA (1992).Google Scholar