Hostname: page-component-54dcc4c588-dbm8p Total loading time: 0 Render date: 2025-10-14T00:56:16.974Z Has data issue: false hasContentIssue false

Deformation Behavior of ReCr Sigma Phase Diffusion Barrier on Ni-based Superalloy

Published online by Cambridge University Press:  26 February 2011

Seiji Miura
Affiliation:
miura@eng.hokudai.ac.jp, Hokkaido Univ., Mat.Sci. and Eng., Kita-13, Nishi-8, Sapporo, 060-8628, Japan, 81-11-706-6347, 81-11-706-6347
Kenji Ohkubo
Affiliation:
ohkubo@lms0-ms.eng.hokudai.ac.jp, Hokkaido Univ., Mat.Sci. and Eng., Kita-13, Nishi-8, Sapporo, 060-8628, Japan
Tetsuo Mohri
Affiliation:
tmohri@eng.hokudai.ac.jp, Hokkaido Univ., Mat.Sci. and Eng., Kita-13, Nishi-8, Sapporo, 060-8628, Japan
Takayuki Yoshioka
Affiliation:
yoshioka@eng.hokudai.ac.jp, Hokkaido Univ., Mat.Sci. and Eng., Kita-13, Nishi-8, Sapporo, 060-8628, Japan
Toshio Narita
Affiliation:
narita@eng.hokudai.ac.jp, Hokkaido Univ., Mat.Sci. and Eng., Kita-13, Nishi-8, Sapporo, 060-8628, Japan
Get access

Abstract

In order to attain a better oxidation resistance of Ni-based superalloys for high performance engines, a ReCr-based sigma-phase diffusion barrier coating between the MCrAlY bond coat (Al reservoir) layer and a Ni-based superalloy substrate has been proposed to suppress the diffusion of Al and other elements. The deformation behavior of TMS82+ superalloy specimens with coating layers composed of an Al-rich surface layer (corresponding to a bond coat) and a ReCr sigma-phase inner layer is investigated. In-situ observation of the bending tests using a Laser scanning confocal microscopy revealed that the crack formation in the Al-rich surface layer(s) on the tension side of the bend specimen occurs at an early stage of bending. On the other hand, small cracks in the sigma-phase layer under the Al-rich surface layer(s) are formed at the slip traces in the Ni-based superalloy single crystal substrate. This suggests a good adhesion between the sigma-phase and the Ni-based superalloy. At the compression side, in both the Al-rich surface layer(s) and the sigma-phase layer no cracking was observed until the Al-rich surface layer(s) shows buckling.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Narita, T., Shoji, M., Hisamatsu, Y., Yoshida, D., Fukumoto, M. and Hayashi, S., Hightemperature corrosion and protection 2000, Science Reviews, (2000) 351.Google Scholar
2. Narita, T., Thosin, K. Z., Fengqun, L., Hayashi, S., Murakami, H., Gleeson, B. and Young, D., Materials and Corrosion, 56 (2005), 923929.Google Scholar
3. Toshio, Narita et al., Materials Science Forum, 502 (2005), 99.Google Scholar
4. Narita, T., Izumi, T., Nishimoto, T., Shibata, Y., Thosin, Kemas Zaini and Hayashi, S., Materials Science Forum, 522'523 (2006), 1.Google Scholar
5. Huang, W. and Chang, Y. A., Materials Science and Engineering, A259 (1999), 110.10.1016/S0921-5093(98)00875-2Google Scholar
6. Villars, P. and Calvert, L. D., “Pearson's handbook of Crystallographic Data for Intermetallic Phases”, ASM, 1985, Materials Park, OH, USA.Google Scholar
7. Ode, T., Journal of the Society of Materials Science, Japan, 44,(1995), 262.Google Scholar
8. Ode, T., Journal of the Materials Science Society of Japan, 34, (1997), 266.Google Scholar
9. Miura, S., Okuno, H., Ohkubo, K. and Mohri, T., MRS Symp. Proc., 842, (2005), 455, MRS, Pittsburgh. Google Scholar
10. Koizumi, Y., Kobayashi, T., Yokokawa, T., Osawa, M., Harada, H., Hino, T., Yoshioka, Y., JOURNAL OF THE JAPAN INSTITUTE OF METALS, 67, (2003), 205.10.2320/jinstmet1952.67.4_205Google Scholar