Acoustic Emission Analysis of Nanoindentation-Induced Fracture Events

Published online by Cambridge University Press:  01 February 2011

Pawel Dyjak
Affiliation:
Mechanics of Advanced Materials Laboratory, Department of Mechanical Engineering, Stony Brook University, Stony Brook, NY 11794–2300
Raman P. Singh
Affiliation:
Mechanics of Advanced Materials Laboratory, Department of Mechanical Engineering, Stony Brook University, Stony Brook, NY 11794–2300
Get access

Abstract

Monitoring of acoustic emission (AE) activity was employed to characterize the initiation and progression of local failure processes during nanoindentation-induced fracture. Specimens of various brittle materials were loaded with a cube-corner indenter and AE activity was monitored during the entire loading and unloading event using an AE transducer mounted inside the specimen holder. As observed from the nanoindentation and AE response, there were fundamental differences in the fracture behavior of the various materials. Post-failure observations were used to identify particular features in the AE signal (amplitude, frequency, rise-time) that correspond to specific types of fracture events. Furthermore, analysis of the parametric and transient AE data was used to establish the crack-initiation threshold, crack-arrest threshold, and energy dissipation during failure. It was demonstrated that the monitoring of AE signals yields both qualitative and quantitative information regarding highly local failure events in brittle materials.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Doener, M.F. and Nix, W.D., Journal of Materials Research 1, 601 (1986).Google Scholar
2. Oliver, W.C. and Pharr, G.M., Journal of Materials Research 7, 1564 (1992).Google Scholar
3. Pharr, G.M., Materials Science and Engineering A-Structural Materials Properties Microstructure and Processing 253, 151 (1998).Google Scholar
4. Harding, D.S., Oliver, W.C., and Pharr, G.M., Proceedings of the 1994 Fall Meeting of MRS (1995).Google Scholar
5. Lawn, B.R., Evans, A.G., and Marshall, D.B., Journal of the American Ceramic Society 63, 574 (1980).Google Scholar
6. Ostojic, P. and McPherson, R., International Journal of Fracture 33, 297 (1987).Google Scholar
7. Yurkov, A.L., Breval, E., and Bradt, R.C., Journal of Materials Science Letters 15, 987 (1996).Google Scholar
8. Bahr, D.F. and Gerberich, W.W., Journal of Materials Research 13, 1065 (1998).Google Scholar