A Nanoindentation Study of Thermally-Grown-Oxide Films on Silicon

Published online by Cambridge University Press:  01 February 2011

Fatih Helvaci
Affiliation:
Dept. of Mechanical Engineering, Thomas J. Watson School of Engineering, State University of New York Binghamton, NY 13902, USA
Junghyun Cho
Affiliation:
Dept. of Mechanical Engineering, Thomas J. Watson School of Engineering, State University of New York Binghamton, NY 13902, USA
Get access

Abstract

We explore the effect of the substrate on mechanical behavior of thin films using a depth-sensing indentation. For this purpose, nanoindentation has been performed on thermally grown silicon oxide films on the silicon substrate. One primary goal of this study is to extract ‘film-only’ mechanical properties from the nanoindentation data by subtracting the substrate effect. It is also shown that elastic modulus of the film is more influenced by the substrate than hardness due to a larger elastic extension beyond a plastically deformed region, as well as a larger elastic mismatch between the SiO2 film and the Si substrate. Further, an inverse analysis of indentation data is proposed to estimate a thickness of thin films. Consequently, this study provides a fundamental understanding in mechanical phenomena of thin films occurring at nanoscales.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Li, X., Diao, D., Bhushan, B., Acta Mater., 45, 44534461 (1997).Google Scholar
2. Choi, Y. and Suresh, S., Acta Mater. 50, 18811893 (2002).Google Scholar
3. Moody, N.R., Medlin, D., Boehme, D., Norwood, D.P., Eng. Frac. Mech., 61, 107118 (1998).Google Scholar
4. Doerner, M.F. and Nix, W.D., J. Mater. Res., 1, 601 (1986).Google Scholar
5. Balk, P., Adv. Mater., 7, 703 (1995).Google Scholar
6. Griscom, D.L., MRS Bull., Jun-Aug 20 (1987).Google Scholar
7. Kern, W. and Rosler, R.S., J. Vac. Sci. Technol., 14, 1082 (1977).Google Scholar
8. Campell, S.A., The Science and Engineering of Microelectronic Fabrication, Oxford University Press, (1996).Google Scholar
9. Pitchon, L., Mourgues, K., Raoult, F., Mohammed-Brahim, T., Kis-Sion, K., Briand, D., Bonnaud, O., Semicond. Sci. Technol., 16, 918 (2001).Google Scholar
10. Hass, G. and Scott, N.W., J. Opt. Soc. Am., 39, 179 (1949).Google Scholar
11. Savage, J.A., Infrared Optical Materials and their Antireflection Coatings, Adam Hilger Ltd., Bristol (1985).Google Scholar
12. Wu, I-Fan, Dottellis, J.B., and Dagenais, M., J. Vac. Sci. Technol. A, 11, 2398 (1993).Google Scholar
13. Saito, K., Uchiyama, Y., and Abe, K., Thin Solid Films, 430, 287 (2003).Google Scholar
14. Pharr, G.M. and Oliver, W.C., MRS Bull., XVII(7) 28 (1992).Google Scholar
15. Joslin, D.L. and Oliver, W.C., J. Mater. Res., 5, 123 (1990).Google Scholar
16. Saha, R. and Nix, W.D., Acta Mater., 50, 23 (2002).Google Scholar
17. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 19, 3 (2004).Google Scholar
18. Helvaci, F., M.S. Thesis, SUNY Binghamton (2004).Google Scholar
19. King, R.B., Int. J. Solids Struct., 23, 1657 (1987).Google Scholar