Nanoindentation Probing of Environmental Effects on Polymer Coating Properties

Published online by Cambridge University Press:  10 February 2011

X. Xia
Affiliation:
ChemE & MatS Department, University of Minnesota, Minneapolis, MN 55455
D. Rowenhorst
Affiliation:
ChemE & MatS Department, University of Minnesota, Minneapolis, MN 55455
K. B. Yoder
Affiliation:
ChemE & MatS Department, University of Minnesota, Minneapolis, MN 55455
L. E. Scriven
Affiliation:
ChemE & MatS Department, University of Minnesota, Minneapolis, MN 55455
W. W. Gerberich
Affiliation:
ChemE & MatS Department, University of Minnesota, Minneapolis, MN 55455
Get access

Abstract

Humidity and temperature control accessories for Hysitron Triboscope have been developed to study the environmental influence on in situ properties of drying coatings. Mechanical properties of drying poly (vinyl alcohol) (PVOH) and poly (vinyl pyrrolidone) (PVP) coatings on silicon wafer were measured under different humidities. The modulus results were compared with outputs of elastic, plastic and viscoelastic theories of indentation testing.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Gutoff, E. B. and Cohen, E. D., Coating and Drying Defects: Troubleshooting Operating Problems, (J. Wiley and Sons, New York, 1995).Google Scholar
2. Errede, L. A., Heinrich, P. J. and Tiers, G. V. D., J. Appl. Polym. Sci., 54, 669 (1994).Google Scholar
3. Crapiste, G. H., Whitaker, S. and Rotstein, E., Chem. Eng. Sci., 43, 2929 (1988).Google Scholar
4. Cairncross, R. A., Jeyadev, S., Dunham, R. F., Evans, K., Francis, L. F. and Scriven, L. E., J. Appl. Polym. Sci., 58, 1279 (1995).Google Scholar
5. Errede, L. A., J. Polym. Sci., Polym. Chem., 28, 857 (1990).Google Scholar
6. Finch, C. A., Polyvinyl Alcohol-Develop, (Wiley, New York, 1992).Google Scholar
7. Oliver, W. C. and Pharr, G. M., J. Mater. Res., 7, 1564 (1992).Google Scholar
8. Sneddon, I. N., Int. J. Eng. Sci. 3, 47 (1965).Google Scholar
9. Gerberich, W. W., Yu, W., Kramer, D., Strojny, A., Bahr, D., Lilleodden, E. and Nelson, J., J. Mater. Res., 13, 421 (1998).Google Scholar
10. Cheng, L., Scriven, L. E. and Gerberich, W. W., in Proceeding of the 4th World Congress on Computational Mechanics, (Buenos Aires, Argentina, 1998).Google Scholar
11. Cheng, L., Xia, X., Yu, W., Scriven, L. E. and Gerberich, W. W., J. Polym. Sci.: Part B: Polym. Phys., 37 (1999).Google Scholar
12. Cheng, L., Scriven, L. E. and Gerberich, W. W., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N. and Baker, S. P. (Mater. Res. Soc. Proc. 522, Warrendal, PA 1998), 193.Google Scholar
13. Cheng, L., private communication.Google Scholar
14. Dibbern-Brunelli, D., Atvars, T. D., Joekes, I. and Barbosa, V. C., J. Appl. Polym. Sci., 69, 645 (1998).Google Scholar
15. Tadokoro, S. Seki and Nitta, I., Bull. Chem. Soc. Jpn., 28, 559 (1955).Google Scholar