Nanoindentation of multilayer PZT/Pt/SiO2 thin film systems on silicon wafers for MEMS applications.

Published online by Cambridge University Press:  01 February 2011

C. Chima-Okereke
Affiliation:
Queen Mary, University of London, England, UK.
M. J. Reece
Affiliation:
Queen Mary, University of London, England, UK.
A. J. Bushby
Affiliation:
Queen Mary, University of London, England, UK.
R. W. Whatmore
Affiliation:
Cranfield University, Cranfield, UK.
Q. Zhang
Affiliation:
Cranfield University, Cranfield, UK.
Get access

Abstract

Nanoindentation is a promising tool for obtaining the elastic properties of thin films. However, no means exists to predict or extrapolate the elastic modulus of the top layer in multilayer systems from experimental data. The mechanical properties of PZT multilayer systems have become increasingly important in applications for MEMS devices. The indentation modulus vs. a/t behaviour of PZT on Pt/SiO2/Si wafer substrate was investigated and compared with a new analytical solution for Herztian indentation of multilayers. Five different PZT film thicknesses were indented (70, 140, 400, 700, 1500 nm), using a 10 μm radius indenter. Good agreement was found between analytical equations and experimental data. However the behaviour of the multilayer system was complex. This makes the deconvolution of film properties difficult for thicknesses less than about 1000 nm.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Algueró, M., Bushby, A. J., Hvizdos, P., Reece, M. J., Whatmore, R. W., Zhang, Q., Mechanical and electromechanical properties of PZT sol-gel thin films measured by nanoindentation, Integrated Ferroelectrics, Vol. 41, (2001), Part ¼, 5362.Google Scholar
2. Fett, T., Munz, D., and Thun, G., Young's Modulus of Soft PZT from partial unloading tests, Ferroelectrics, Vol. 274, (2002), p 6781.Google Scholar
3. Menčík, J., Munz, D., Quandt, E., Weppelmann, E.R., and Swain, M.V., Determination of elastic modulus of thin layers using nanoindentation; J. Mater. Res., Vol. 12, No. 9, Sep 1997, 24752484.Google Scholar
4. Hsueh, C-H., and Miranda, P., Master curves for Hertzian indentation on coating/substrate systems, J. Mater. Res., Vol.19, No.1, (2004), 94100.Google Scholar
5. Kim, J. – K., Kim, N. – K., Park, B. – O., Effects of ultrasound on microstructure and electrical properties of Pb (Zr0.5 Ti0.5)O3 thin films prepared by sol–gel method; Materials Letters 39 (1999) 280 – 286.Google Scholar
6. Swadener, J. G., and Pharr, G. M., Indentation of elastically anisotropic half-spaces by cones and parabolae of revolution; Phil. Mag. A, Vol. 81, No.2, (2001) 447466.Google Scholar
7. Bushby, A. J., Nano-indentation using spherical indenters; Nondestructive testing and evaluation, Vol. 17, (2001), 213234.Google Scholar
8. Field, J.S. and Swain, M.V., A simple predictive model for spherical indentation; J. Mater. Res., Vol.8, No.2, (1993), 297306.Google Scholar