MODELING OF NANOINDENTATION AND MICROSTRUCTURAL DUCTILE BEHAVIOR IN METALLIC MATERIAL SYSTEMS

Published online by Cambridge University Press:  01 February 2011

Jeong Beom Ma
Affiliation:
Department of Mechanical and Aerospace Engineering, North Carolina State University, Raleigh, NC 27695–7910
W. Ashmawi
Affiliation:
Department of Mechanical and Aerospace Engineering, North Carolina State University, Raleigh, NC 27695–7910
M. A. Zikry
Affiliation:
Department of Mechanical and Aerospace Engineering, North Carolina State University, Raleigh, NC 27695–7910
D. Schall
Affiliation:
Department of Materials Science and Engineering North Carolina State University, Raleigh, NC 27695–7910
D. W. Brenner
Affiliation:
Department of Materials Science and Engineering North Carolina State University, Raleigh, NC 27695–7910
Get access

Abstract

Specialized large-scale computational finite-element and molecular dynamic models have been used to understand and predict how dislocation density emission and contact stress fields due to nanoindentation affect inelastic deformation evolution at scales that span the molecular to the continuum level in ductile crystalline systems. Dislocation density distributions and local stress fields have been obtained for different crystalline slip-system and grain-boundary orientations. The interrelated effects of grain-boundary interfaces and orientations, dislocation density evolution and crystalline structure on indentation inelastic regions have been investigated.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Suresh, S., Nieh, T.G., and Choi, B.W. Scripta Mater. 9, 41951 (1999).Google Scholar
2. Gerberich, W.W., Tymiak, N.I., Grunlan, J.C., Horstemeyer, M.F., Baskes, M.I. J Appl. Mech. 69, 433 (2002).Google Scholar
3. Hasnaoui, A., Derlet, P.M., and Van Swygenhoven, H. Acta Mater. 52, 2251 (2004).Google Scholar
Lilleodden, , Zimmerman, E.T., Foiles, J.A., and Nix, W.D., J. Mech. Phys. Solids 51, 901 (2003).Google Scholar
4. Zikry, M. A. and Kao, M., J. Mech. Phys. Solids 44, 1765 (1996).Google Scholar
5. Ashmawi, W. M. and Zikry, M. A., J. Computer-Aided Mater. Design, 7, 55 (2000).Google Scholar
6. Kameda, T. and Zikry, M. A., Int. J. Plasticity 14, 689 (1998).Google Scholar
7. Schall, J.D. and Brenner, D.W., Schall, , J. Mater. Res. 19, 3172 (2004).Google Scholar
8. Randle, V., Acta Mater., 46, 1459 (1997).Google Scholar
9. Ashmawi, W.M. and Zikry, M.A., Mater. Sci. Engng. A 343, 1 (2002).Google Scholar
10. Zikry, M. A., Comput. Struct. 50, 337 (1994).Google Scholar