Hostname: page-component-54dcc4c588-64p75 Total loading time: 0 Render date: 2025-10-14T06:06:30.559Z Has data issue: false hasContentIssue false

Microbridge Nanoindentation Testing of Plasma-Enhanced Chemical Vapor Deposited Silicon Oxide Films

Published online by Cambridge University Press:  01 February 2011

Zhiqiang Cao
Affiliation:
Department of Manufacturing Engineering, Boston University, Boston, MA 02215, USA
Tong-Yi Zhang
Affiliation:
Department of Mechanical Engineering, Hong Kong University of Science and Technology, Clear Water Bay, Kowloon, Hong Kong, China
Xin Zhang
Affiliation:
Department of Manufacturing Engineering, Boston University, Boston, MA 02215, USA
Get access

Abstract

Plasma-enhanced chemical vapor deposited (PECVD) silane-based oxides (SiOx ) have been widely used in both microelectronics and MEMS (MicroElectroMechanical Systems) to form electrical and/or mechanical components. In this paper, a novel nanoindentation-based microbridge testing method is developed to measure both the residual stresses and Young's modulus of PECVD SiOx films. Our theoretical model employed a closed formula of deflection vs. load, considering both substrate deformation and the residual stresses in the thin films. In particular, the non-negligible residual deflection caused by excessive compressive stresses was taken into account. Freestanding microbridges made of PECVD SiOx films were fabricated using bulk micromachining techniques. To simulate the thermal processing in device fabrication, these microbridges were subjected to rapid thermal annealing (RTA) up to 800°C. A microstructure-based mechanism was applied to explain the experimental results of the residual stress changes in PECVD SiOx films after thermal annealing.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Madou, M., Fundamentals of Microfabrication: The Science of Miniaturization, 2nd ed. (CRC Press, Boca Raton, 2002).Google Scholar
2. Ohring, M., The Material Science of Thin Films (Academic Press, New York, 1992).Google Scholar
3. Brotzen, F. R., Int. Mater. Rev., 39, 24 (1994).Google Scholar
4. Pharr, G. M. and Oliver, W. C., MRS Bull., XVII, 28 (1992).Google Scholar
5. Schweitz, J., MRS Bull., XVII, 34 (1992).Google Scholar
6. Vlassak, J. J. and Nix, W. D., J. Mater. Res., 7, 3242 (1992)Google Scholar
7. Zhang, T.-Y. et al, Acta Mater. 48, 2843 (2000).Google Scholar
8. Su, Y.-J. et al, Acta Mater. 48, 4901 (2000).Google Scholar
9. Xu, W.-H. and Zhang, T.-Y., Appl. Phys. Lett. 83, 1731 (2003).Google Scholar
10. Hirth, J. P. and Lothe, J., Theory of Dislocations, 2nd ed. John Wiley, New York, 1982.Google Scholar
11. Cao, Z. and Zhang, X., J. Appl. Phys., 96, 4273 (2004).Google Scholar