Hostname: page-component-54dcc4c588-ff9ft Total loading time: 0 Render date: 2025-10-10T00:18:58.072Z Has data issue: false hasContentIssue false

Mechanical Behaviour of Eutectic Superalloys

Published online by Cambridge University Press:  15 February 2011

M. McLean*
Affiliation:
Division of Materials Applications, National Physical Laboratory, Teddington, Middlesex TWIt OLW, UK
Get access

Extract

The mechanical properties of in-situ composites intended for use as gas turbine materials are reviewed. Particular emphasis is placed on the current understanding of strengthening and fracture mechanisms of these materials. The need to modify current methods of data representation, that have been developed for more conventional materials, in order to improve property extrapolation and design procedures are highlighted.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1982

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Bibring, H. - Proceedings of Conference on In-Situ Composites I, National Materials Advisory Board Publication 308–II, p. 1, Washington DC. January 1973.Google Scholar
2. Lawley, A. - Proceedings of Conference on In-Situ Composites II, edited by Jackson, M.R. et al. ., p. 451, Xerox Individualised Publishing, Lexington, Mass., 1976 Google Scholar
3. Stoloff, N.S. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , Ginn and Company, Lexington, Mass., 1979 Google Scholar
4. Kelly, A. - “Strong Solids”, Oxford University Press, Oxford, 1973.Google Scholar
5. Thompson, E.R., George, F.D. and Breinan, E.M. - Proceedings of Conference on In-Situ Composites I, National Materials Advisory Board Publication. 308–II, p. 71, Washington, DC. (1973).Google Scholar
6. Bullock, E., P.N. Quested and M. McLean, Acta Met.25, 333 (1977).Google Scholar
7. Walter, J.L., this volume.Google Scholar
8. Chadwick, G.A., Acta Met. 24, 1137 (1976).Google Scholar
9. McDanels, D., Signorelli, R.A. and Weeton, J.W., NASA Rept. No TND-4173 (1967).Google Scholar
10. Miles, D.E., Bullock, E. and McLean, M. - Proceedings of Conference on In-Situ Composites II, edited by Jackson, M.R. et al. , p. 539, Xerox Individualised Publishing, Lexington, Mass., (1976).Google Scholar
11. McLean, M., Proc. Roy. Soc. London. 371A, 279 (1980).Google Scholar
12. McLean, M., Proc. Roy. Soc. London. 373A, 93 (1980).Google Scholar
13. Khan, T., Stohr, J.F. and Bibring, H.. - “Superalloys 1980”, Proceedings of 4th Int. Symp. on Superalloys, edited by Tien, J.K. et al. , p American Society for Metals, Metals Park, Ohio, (1980).Google Scholar
14. Woodford, D.A. - Metall. Trans. 8A, 639 (1977).Google Scholar
15. Khan, T. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 378, Ginn and Co., Lexington, Mass., 1979.Google Scholar
16. Bullock, E., Quested, P.N. and McLean, M. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 420, Ginn and Co., Lexington, Mass., 1979.Google Scholar
17. Miles, D.E. and McLean, M., Metal Science 11, 563 (1977).Google Scholar
18. Giglotti, M.F.X., Jackson, M.R., Yang, S.W., Henry, M.F. and Woodford, D.A.-this volume.Google Scholar
19. Scarlin, R.B. and Speidel, M.O., Boveri, Brown et al. , Baden-Switzerland - Final Report of COST 50 programme CH3/4, July 1976.Google Scholar
20. Henderson, P.J. and McLean, M., Acta Met. to be published.Google Scholar
21. Breinan, E.M., Thompson, E.R. and Lemkey, F.D. - Proc. of Conf. on In-Situ Composites I, p. 201, National Materials Advisory Board Publication 308–11, Washington, DC, 1973.Google Scholar
22. Woodford, D.A. - Proceedings of Conference on In-Situ Composites II, edited by Jackson, M.R. et al. , p. 211, Xerox Individualised Publishing, Lexington, Mass., 1976.Google Scholar
23. Woodford, D.A. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 410, Ginn and Co., Lexington, Mass., 1979.Google Scholar
24. Bruch, C.A., Harrison, R.W., Gigliotti, M.J.X., Henry, M.F., Haubert, R.C. and Gay, C.H. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 258, Ginn and Co., Lexington, Mass., 1979.Google Scholar
25. Bullock, E., Quested, P.N. and McLean, M. - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 420, Ginn and Co., Lexington, Mass., 1979.Google Scholar
26. Sahm, P.R. and Schübert, Fl - Proceedings of Conference on In-Situ Composites III, edited by Walter, J.L. et al. , p. 268, Ginn and Co., Lexington, Mass., 1979.Google Scholar