Hostname: page-component-54dcc4c588-mz6gc Total loading time: 0 Render date: 2025-10-09T01:53:08.517Z Has data issue: false hasContentIssue false

In Situ Etch Rate Measurements by Alpha-Particle Energy Loss

Published online by Cambridge University Press:  10 February 2011

Y. Levy
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
A. Ballestad
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
M. Davies
Affiliation:
Institute for Microstructural Sciences, National Research Council of Canada, Ottawa, ON K1A 0R6, Canada
Y. Feng
Affiliation:
Institute for Microstructural Sciences, National Research Council of Canada, Ottawa, ON K1A 0R6, Canada
I. Kelson
Affiliation:
School of Physics and Astronomy The Raymond and Beverly Sackler Faculty of Exact Sciences, Tel Aviv University, Tel Aviv 69978, Israel
W.J. Mandeville
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
V. Pacradouny
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
A. Schmalz
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
T. Tiedje
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
J.F. Young
Affiliation:
Department of Physics and Astronomy, University of British Columbia, Vancouver, BC V6T 1Z4, Canada
Get access

Abstract

When alpha-particles pass through thin films they lose an amount of energy proportional to the film thickness with the proportionality constant depending on the film composition. Thus, by measuring this energy loss one can determine the film thickness. We have applied this technique to measurements of the etch rate of various III-V semiconductor layers grown by molecular beam epitaxy. Prior to film growth, GaAs substrates were recoil-implanted with the alpha-emitting 224Ra isotope by exposure to a 5µCi source of 228Th. The implanted isotope decays with a half-life of 3.7 days, which allows measurements to be done for up to about two weeks after implantation. Following growth, the samples were etched in an electron cyclotron resonance etcher using a Cl2/BCl3/Ar gas mixture. As the film is etched the energy of the alpha-particles emitted from the surface increases. By introducing a high resolution Si detector into the etcher we are able to measure changes in the alpha-emission spectrum without removing the sample from the etcher. Thickness changes with an uncertainty of 5–10nm are obtained in 5 minute measurements at the end of each etch step. Some of the samples were also measured by SEM, yielding results in good agreement with values obtained by the alpha-particle measurements. As an example of an application of the technique we will describe measurements of the temperature dependence of the etch rate of GaAs in the 15–150 °C temperature range using optical bandgap thermometry to determine the substrate temperature. In a second example, we explore the application of the technique to etch rate of short pitch (250–500nm) grating. In this case the shape of the alpha-spectrum is sensitive to the profile of the etched trenches.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Shul, R.J., Howard, A.J., Vartuli, C.B., Barnes, P.A. and Seng, W., J. Vac. Sci. Technol. A14, (3) 1102 (1996).10.1116/1.580276Google Scholar
2. Sah, R.E., Ralston, J.D., Weisser, S. and Eisele, K., Appl. Phys. Lett. 67, 927 (1995).10.1063/1.114697Google Scholar
3. Snyder, P.G., lanno, N.J., Wigers, B., Pittal, S., Johs, B. and Woollam, J.A., J. Vac. Sci. Technol. B 13, (6) 2255 (1995).10.1116/1.588059Google Scholar
4. Laaksonen, R. Tapani, Semiconductor International, 20, (8) 277 (1997).Google Scholar
5. Kahaian, D.J., Thomas, S. III and Pand, S.W., J. Vac. Sci. Technol. B13, (2) 253 (1995).10.1116/1.588360Google Scholar
6. Franz, G., Hoyler, C. and Kaindl, J., J. Vac. Sci. Technol. B 14, (1 126 (1996).10.1116/1.589039Google Scholar
7. Beaudoin, M. et al. , Appl. Phys. Lett. 72, 3288 (1998).Google Scholar
8. Kelson, I., Levy, Y. and Redmard, E., J. Phys D: Appl. Phys. 28, 100 (1995).10.1088/0022-3727/28/1/016Google Scholar
9. Kelson, I. et al. , J. Phys D: Appl. Phys. 30, 131 (1997).10.1088/0022-3727/30/1/016Google Scholar
10. Lederer, C.M. and Shirley, V.S. (ed), Table of Isotopes, 7h ed. (Wiley Intercsience, New York, 1977).Google Scholar
11. Weilmeier, M.K., Colbow, K.M., Tiedje, T., Buuren, T. van and Xu, L., Can. J. Phys. 69, 422 (1991).10.1139/p91-068Google Scholar
12. Johnson, S.R., Lavoie, C., Niessen, M.K., Tiedje, T., US Patent No. 5,388,909 (1995).Google Scholar