High Temperature Deformation of AlN/CrN Multilayers using Nanoindentation

Published online by Cambridge University Press:  01 February 2011

F. Giuliani
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Pembroke Street, Cambridge, CB2 3QZ, UK.
A. Goruppa
Affiliation:
Teer Coatings Ltd., West Stone House, Berry Hill Industrial Estate, Droitwich, Worcestershire, WR9 9AS, UK.
S. J. Lloyd
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Pembroke Street, Cambridge, CB2 3QZ, UK.
D. Teer
Affiliation:
Teer Coatings Ltd., West Stone House, Berry Hill Industrial Estate, Droitwich, Worcestershire, WR9 9AS, UK.
W. J. Clegg
Affiliation:
Department of Materials Science and Metallurgy, University of Cambridge, Pembroke Street, Cambridge, CB2 3QZ, UK.
Get access

Abstract

The aim of this paper is to investigate the deformation behaviour of an AlN/CrN multilayer with wavelengths varying from 6–400 nm, deposited on M42 tool steel and how this varies as the temperature is increased to 500 °C. These measurements have been correlated with changes in deformation patterns using cross-sectional transmission electron microscopy, where sections have been prepared directly through the indents.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Sproul, W.D.. Surf. Coat. Tech. 86–87, 170 (1996)Google Scholar
2. Shinn, M. and Barnett, S.A.. Appl. Phys. Lett. 64(1), 61 (1994)Google Scholar
3. Anderson, P.M., Foecke, T. and Hazzledine, P.M.. MRS Bull. 24(2), 27 (1999)Google Scholar
4. Clegg, W.J., Giuliani, F., Long, Y., Lloyd, S.J., ‘Hardening in multilayer ceramics’, in Ceramic Matrix Composites: Microstructure/Property Relationship, edited by Low, I. M., Woodhead Publishing, Cambridge, (in press 2005)Google Scholar
5. Monaghan, D P et al. Surf. Coat. Tech, 59, 21 (1993)Google Scholar
6. Oliver, W.C. and Pharr, G.M.. J. Mater. Res. 7, 1564 (1992)Google Scholar
7. Langford, R.M. and Pettford-Long, A.K.. J. Vac. Sci. Techn. A, 19(5), 2186 (2001)Google Scholar
8. Ji, X., Lau, S., Yu, G., Zhong, W., Wang, Y. and Tay, B. J. Phys. D, 36, 25432547 (2003)Google Scholar
9. Lousa, A., et al. Surf. Coat. Tech., 146–147, 146 (2001)Google Scholar
10. Kral, C., Lengauer, W., Rafaja, D. and Ettmayer, P., J. Alloy. Comp. 265, 215233 (1998)Google Scholar
11. Yonenaga, . MRS Internet. J. Nitride Semicond. Res. Soc, Vol. 7(6) (2002)Google Scholar