Hostname: page-component-84c44f86f4-pqzqq Total loading time: 0 Render date: 2025-10-14T12:39:32.589Z Has data issue: false hasContentIssue false

Fracture and Fractography of Ordered Ni4Mo

Published online by Cambridge University Press:  26 February 2011

H. P. Kao
Affiliation:
Chung-Shan Institute of Science and Technology, Lung-Tan, Taiwan, Republic of China
C. R. Brooks
Affiliation:
Materials Science and Engineering Department, The University of Tennessee, Knoxville, TN 37996-2200
M. Sanganeria
Affiliation:
Materials Science and Engineering Department, The University of Tennessee, Knoxville, TN 37996-2200
Get access

Abstract

The domain structure of the alloy Ni-20 at. % Mo depends upon the heat treatment below the critical temperature (868°C). Upon aging around 750–850°C, initially a very fine domain structure forms inside the a grains, which then coarsens, and then migration of these boundaries occurs with a coarser domains structure behind them. In the ordered condition, the alloy is very brittle. Fractographs are presented which correlate the fracture morphology to the microstructures of the ordered alloy, showing that fracture occurs along the migrated, former α grain boundaries.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1989

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Stoloff, N .S., Int. Metals Rev. 29, 210 (1984).Google Scholar
2. Brooks, C. R., Spruiell, J. E. and Stansbury, E. E., Int. Metals Rev. 29, 210 (1984).Google Scholar
3. Kao, H. P., Vasudevan, K. and Brooks, C. R., in Proc. 44th Annual Meeting Elect. Mic. Soc. Am., edited by Bailey, G.W., (San Francisco Press, San Francisco 1986) p. 560.Google Scholar
4. Brooks, C. R. and Sanganeria, M., Scripta Met., 22, 1683 (1988).CrossRefGoogle Scholar
5. Kao, H. P. and Brooks, C. R., Scripta Met. 20, 1561, (1986).CrossRefGoogle Scholar
6. Choudhury, A., Kao, H. P., Brooks, C. R. and White, C. L., Scripta Met. 22, 1057, (1988).CrossRefGoogle Scholar