Hostname: page-component-54dcc4c588-2bdfx Total loading time: 0 Render date: 2025-10-14T00:54:15.314Z Has data issue: false hasContentIssue false

Experimental Analysis of Viscoelastic Behavior in Nanoindentation

Published online by Cambridge University Press:  10 February 2011

A. Stroiny
Affiliation:
Chemical Engineering and Materials Science Department, University of Minnesota, Minneapolis, MN 55455
W. W. Gerberich
Affiliation:
Chemical Engineering and Materials Science Department, University of Minnesota, Minneapolis, MN 55455
Get access

Abstract

Conventional analysis of load displacement curves in nanoindentation experiments determine modulus by using the elastic portion of the unloading slope or power law fitting the unloading slope. For polymeric materials, however, this analysis is not adequate because they behave viscoelastically. In companion research, L. Cheng has developed analytical models for flat tip and spherical tip indentation using a three element Kelvin-Voigt model, with a spring in series with a parallel dashpot and a spring for compressible and incompressible materials.

Incompressible (v=0.5) polydimethylsiloxane coatings with thicknesses of 2 and 78 microns, a compressible (v=0.33) bulk polystyrene (PS) and a 16 Jim styrene-acrylate block copolymer coating (v=0.33) have been used to verify the models. The polymers were indented using flat tip and spherical tip indenters with a nanoindentation apparatus in creep (constant load) and relaxation modes (constant depth). The data was fit to the analytical models using a non-linear least squares fit algorithm varying three parameters. In general the fitted elastic and shear moduli compared favorably with conventional rheological and mechanical measurements on the same bulk polymers. However, it appears that the agreement for the thin film analysis can be improved by taking the hydrostatic pressure dependence of the modulus and substrate effects into consideration.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Doerner, M. F., Nix, W. D., J. of Mat. Res., 1(4), 601609 (1986)Google Scholar
2. Oliver, W. C., Pharr, G. M., J. of .Mater. Res.,7(6), 15641583 (1992)Google Scholar
3. Wu, T. W., J. Mater. Res., 6(2) 407426(1991)Google Scholar
4. Mencik, J., Swain, M. V., Materials Forum, 18, 277288(1994)Google Scholar
5. Arruda, E. M., Boyce, M. C., Int. J. of Plasticity, 9, pp. 697720 (1993)Google Scholar
6. Cheng, L., Scriven, L. E., Gerberich, W. W., submitted to WCCM IV, Argentina, 1998 Google Scholar
7. in house testing by Dow ComingGoogle Scholar
8. Hellwege, K. H., Knappe, W. ,Paul, F., Semjonow, V., Rheol. Acta., 6, 165 (1967)Google Scholar
9. Patterson, M. S., J. Appl. Phys., 35(1), 176179 (1964)Google Scholar
10. Fillers, R. W., Tschoegl, N. W., Trans. Soc. Rheol., 21, 51(1977)Google Scholar