Characterization of NiTi Shape Memory Wires by Differential Scanning Calorimetry and Transmission X-ray Diffraction

Published online by Cambridge University Press:  25 February 2011

Ming-Yuan Kao
Affiliation:
Johnson Controls, Inc., P.O.Box 591, Milwaukee, WI 53201
Sepehr Fariabi
Affiliation:
Johnson Controls, Inc., P.O.Box 591, Milwaukee, WI 53201. Currently with ACS Inc., P.O.Box 58167, Santa Clara, CA 95052
Paul E. Thoma
Affiliation:
Johnson Controls, Inc., 507 E. Michigan Street, Milwaukee, WI 53202
Husnu Ozkan
Affiliation:
Marquette University, Milwaukee, WI 53233. Currently with Middle East Technical University, Ankara, Turkey 06531
Louis Cartz
Affiliation:
Marquette University, Milwaukee, WI 53233
Get access

Abstract

The reversible transformations between the Austenite (A) and Martensite (M) phases of NITI shape memory wires having a 78°C austenlte finish temperature (950°C annealed) were studied In the cold work and heat treatment ranges between 14 to 62% and 400 to 525°C respectively. The ranges of peak Transformation Temperatures (TI), determined by Differential Scanning Calorimetry (DSC) at a 10°C/min rate, were found to be 56 to 75°C, -28 to 33°C, and 38 to 52°C for the respective high temperature A, low temperature M, and the Intermediate Rhombohedral (R) phases. The degree of cold work and heat treatment had significant effects on the TT of NITI wires. The peak TT of A and M decreases with Increasing cold work. Except for the 14% cold worked wires, the peak TT Increases with Increasing heat treatment temperature for M, and Increases with Increasing heat treatment temperature for A for temperatures higher than 450°C. The peak IT of R Increases with Increasing cold work and decreasing heat treat temperature.

Using MoKα radiation, transmission x-ray diffraction analysis was utilized to determine the phases at room temperature on wires thinned down to 0.05 to 0.01 mm in diameter. The diffraction patterns of body-centered cubic austenite (132) and monodlinic martenslte (B19) for NITi were both Identified. In addition, extra diffraction lines observed for various samples were tentatively assigned to M and the Intermediate R-phase. Depending on the thermal history and the processing conditions, the NITI wires consist of either a pure M, a mixture of A and R, or a mixture of A, R, and M at room temperature.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Todoroki, T. and Tamura, H., “Effect of Heat Treatment after Cold Working on the Phase Transformation in TiNi Alloy”, Trans. Japan Inst. Met., 28 (2) (1987) 83.CrossRefGoogle Scholar
2. AbuJudom, D. N., Thoma, P. E., and Fariabi, S. (the order of names was changed to Farlabl, S., AbuJudom, D. N., and Thoma, P. E. by letter to the editor after the Proceedings were published), “The Effect of Cold Work and Heat Treatment on the Phase Transformations of Near Equlatomic NITI Shape Memory Alloy”, Materials Science Forum, Proceedings of ICOMAT-89, Sydney, Australia, July 1989, 56–58 (1990) 565.Google Scholar
3. Thoma, P. E., AbuJudom, D. N., and Fariabi, S., “Method for Producing a Shape Memory Alloy Member Having Specific Physical and Mechanical Properties”, U. S. Patent No. 4,881,981, November 21, 1989.Google Scholar
4. Farlabi, S., McKlnney, B. L., and Hodgson, D. E., “Mechanical Characterization of Ti-50.1% Ni After Various Heat Treatment Using a Statistically Aided Testing Program”, Materials Science Forum, Proceedings of ICOMAT-89, Sydney, Australia, July 1989, 56–58 (1990) 753.Google Scholar
5.Powder Diffraction File (PDF), PDF's 18-899 & 19-850 for austenite and 27-344 & 35-1281 for martensite, Joint Committee on Powder Diffraction Standard-Intemational Center for Diffraction Data, Swarthmore, PA 1980.Google Scholar
6. Wang, F. E., Pickart, S. J., and Alperin, H. A., “Mechanism of the TINI Martensitic Transformation and the Crystal Structures of TiNi-II and TiNi-III Phases”, J. Appl. Phys. 43 (1972) 97.CrossRefGoogle Scholar
7. Ung, H. C. and Kaplow, R., “Phase Transitions and Shape Memory in NiTi”, Met. Trans., 11A (1980) 77.Google Scholar
8. Miyazaki, S. and Otsuka, K., “Deformation and Transition Behavior Associated with the R-phase In Ti-Ni Alloys”, Met. Trans., 17A (1986) 53.CrossRefGoogle Scholar
9. Miyazaki, S. and Wayman, C. M., “The R-phase Transition and Associated Shape Memory Mechanism in Ti-Ni Single Crystals”, Acta. Met. 36(1) (1988) 181.Google Scholar
10. Thoma, P. E. and Fariabi, S., to be presented at ICOMAT-92, Monterey, CA, July 20-24, 1992.Google Scholar