Lean duplex stainless steels – The role of molybdenum additionon pitting corrosion of concrete reinforcements

Published online by Cambridge University Press:  01 December 2011

T. Mesquita
Affiliation:
Ugitech Research Center, Avenue Paul Girod, 73403 Ugine Cedex, France. e-mail: thiago-jose.mesquita@lepmi.grenoble-inp.fr LEPMI – INP Grenoble, rue de la Piscine, 38402 St. Martin d’Hères, France
E. Chauveau
Affiliation:
Ugitech Research Center, Avenue Paul Girod, 73403 Ugine Cedex, France. e-mail: thiago-jose.mesquita@lepmi.grenoble-inp.fr
M. Mantel
Affiliation:
Ugitech Research Center, Avenue Paul Girod, 73403 Ugine Cedex, France. e-mail: thiago-jose.mesquita@lepmi.grenoble-inp.fr
N. Kinsman
Affiliation:
International Molybdenum Association, 4 Heathfield Terrace, London, UK
R.P. Nogueira
Affiliation:
LEPMI – INP Grenoble, rue de la Piscine, 38402 St. Martin d’Hères, France
Get access

Abstract

The use of stainless steels as concrete reinforcement is becoming increasingly popular incoastal and marine constructions in order to prevent corrosion induced by chloride ionspenetrating into the concrete. In these highly aggressive situations, the lean duplexstainless steels have been extensively employed due to their high mechanical and corrosionresistances. However, the influence of Mo addition on pitting corrosion resistance ofthese steels is not clearly understood in alkaline chloride conditions even if thiselement is widely associated to an increasing corrosion resistance in acidic and neutralenvironments. Therefore, understanding Mo mechanism on corrosion resistance in alkalinemedia is hence of major importance to the setting of optimized alloy composition. Thepresent work aims to study the effect of Mo addition on pitting corrosion properties oflean duplex stainless steels in alkaline environments (concrete). The results arediscussed with respect to the influence of Mo addition on pitting potential for twoindustrial duplex alloys (1.4362 and 1.4462) in several aggressive media mainly insynthetic, chlorinated and carbonated solution simulating concrete pore environments (pH10solution with carbonates and chlorides ions). In order to establish the real role of Moaddition on lean duplex corrosion and passivation properties, the corrosion behaviors oftwo specific laboratory lean duplex alloys, which the only difference between then is theamount of Mo (0 and 3% wt. Mo), are also studied. Furthermore, scanning electronicmicroscopy (SEM) was used to verify which phase of duplex microstructure (ferritic oraustenitic) is mostly susceptible to the pit nucleation in these corrosion conditions asthe role of Mo is probably different to each simple phase.

Information

Type
Research Article
Copyright
© EDP Sciences, 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

E. Chauveau, T. Sourisseau, B. Dermelin, M. Mantel, MEDACHS 08, International Conference in Coastal and Marine Environments, 2008
Addari, D., Elsener, B., Rossi, A., Electrochim. Acta E 53 (2008) 27
Abbott, C.J., Concrete E 31 (1997) 5
Gedge, G., J. Constr. Steel Res. E 64 (2008) 11
F. Zhang, J. Pan, C. Lin, Corrosion Sci. (2009)
Zhang, L., Jiang, Y., Deng, B., Zhang, W., Xu, J., Li, J., Materials Characterization E 60 (2009) 12
R.N. Gunn, Abingtion Publishing, Cambridge England, 1999
Garfias-Mesias, L.F., Sykes, J.M., Tuck, C.D.S., Corrosion Sci. E 38 (1996) 8
T.J. Mesquita, E. Chauveau, M. Mantel, N. Kinsman, R.P. Nogueira, Stainless Steel in Rio - Inox 2010, 10th Brazilian Stainless Steel Conference – International Edition, 2010
Zhang, L., Jiang, Y., Deng, B., Zhang, W., Xu, J., Li, J., Electrochim. Acta E 54 (2009) 23
Pardo, A., Merino, M.C., Coy, A.E., Viejo, F., Arrabal, R., Matykina, E., Corrosion Sci. E 50 (2008) 3
Pardo, A., Merino, M.C., Coy, A.E., Viejo, F., Arrabal, R., Matykina, E., Corrosion Sci. E 50 (2008) 6
Deng, B., Wang, Z., Jiang, Y., Wang, H., Gao, J., Li, J., Electrochim. Acta E 54 (2009) 10
Deng, B., Jiang, Y., Gong, J., Zhong, C., Gao, J., Li, J., Electrochim. Acta E 53 (2008) 16
Gao, J., Jiang, Y., Deng, B., Zhang, W., Zhong, C., Li, J., Electrochim. Acta E 54 (2009) 24
Bastos, I.N., Tavares, S.M., Dalard, F., Nogueira, R.P., Scripta Materialia E 57 (2007) 10